Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 282 °C | 540 °F | Unannealed; Flatwise; ISO 75-2/A |
Solvay Specialty Polymers Amodel® AS-1945 HS Polyphthalamide (PPA), 45% Glass Fiber Amodel® AS-1945 HS is a 45% glass reinforced grade of polyphthalamide (PPA) resin developed specifically for improved performance in a 50/50 ethylene glycol and water environment. This material e.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 282 °C | 540 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA LNP* THERMOCOMP* UF006H is a compound based on Polyphthalamide resin containing 30% Glass Fiber. Added feature of this grade is: Healthcare. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 282 °C | 540 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOCOMP UF006H PPA (Asia Pacific) LNP* Thermocomp* UF006H is a compound based on Polyphthalamide resin containing Glass Fiber. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 282 °C | 540 °F | ASTM D648A |
Sumitomo Bakelite North America 2004B Glass Reinforced Hardware Grade Epoxy Epoxy is the premier material for military firewall connectors.Information provided by Sumitomo Bak North America, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America E 3938A Hardware Grade Epoxy Fiberglass reinforced epoxy molding compound with excellent dimensional stability, good strength and excellent electrical insulation properties.Information provided by Vyncolit, a Sumitomo Bak Group.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ISO 75 A |
Sumitomo Bakelite North America RX® 640 Fiberglass Reinforced Phenolic Resole RX 640 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-5.Information supp.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America RX® 643 Fiberglass Reinforced Phenolic RX 643 is a fiberglass reinforced, ammonia-free, phenolic resole compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type GPI-10.Information pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ISO 75 A |
Sumitomo Bakelite North America RX® 660 Fiberglass Reinforced Phenolic Novolac RX 660 is a fiberglass reinforced phenolic molding compound, with good dimensional stability and good strength at elevated temperatures. Meets ASTM D-5948 Type MFH.Information supplied by Sumitom.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America FM 4005X4648 Fiberglass Reinforced Phenolic Novolac FM 4005X4648 a fiberglass reinforced phenolic novolac molding compound formulated to increase thermal conductivity and electrical conductance. This material also exhibits low post mold shrinkage.In.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 282 °C | 540 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL BK337 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 282 °C | 540 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL BK337 Polyphthalamide (PPA)
(Unverified Data**) Zytel® HTNFR52G30BL BK337 is a 30% glass reinforced, flame retardant, lubricated high performance polyamide resin that has been developed for connector applications.Information provided by DuPont P.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America Epiall® 1914A Short Glass Fiber Reinforced Epoxy Epiall 1914A is a short fiberglass reinforced epoxy molding compound, with excellent dimensional stability, good strength properties and good electrical insulation properties.Information provided by.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America FM 4004 Fiberglass and Mineral Reinforced Phenolic Novolac FM 4004 is a fiberglass and mineral reinforced phenolic novolac compound. This compound exhibits excellent dimensional stability and good strength at elevated temperatures, and conforms to the requ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ASTM D648A |
Sumitomo Bakelite North America FM 4005X4649 Fiberglass Reinforced Phenolic Novolac FM 4005X4649 a fiberglass reinforced two-step phenolic molding compound formulated to increase thermal conductivity, to provide static dissipation and good wear resistance to abrasive media.Informat.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ISO 75 A |
Sumitomo Bakelite North America RX® 790 Fiberglass Reinforced Phenolic Novolac RX 790 is a fiberglass reinforced phenolic novolac compound, featuring a good balance of strength and toughness. Information supplied by Sumitomo Bak North America. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ISO 75 A |
Sumitomo Bakelite North America RX® 852 Novolac Phenolic Fiberglass reinforced phenolic novolac compound with good dimensional stability and good strength at elevated temperatures.Information provided by Vyncolit, a Sumitomo Bak Group |
|||
Deflection Temperature at 1.8 MPa (264 psi) | >= 282 °C | >= 540 °F | Post Baked; ISO 75 A |
Sumitomo Bakelite North America RX® 865M Novolac Phenolic Fiberglass reinforced phenolic novolac compound featuring dimensional stability, moderate impact resistance, good strength and modulus.Information provided by Vyncolit, a Sumitomo Bak Group |