Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | Unannealed; ISO 75-2/A |
PolyOne OnForce™ LFT PP-50LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer) PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | ISO 75Af |
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded
( AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
PolyOne Lubri-Tech™ AT-000/20T Copolymer Acetal - 20% PTFE Lubricated
(discontinued **) Data provided by PolyOne. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 - 177 °C | 310 - 351 °F | Average value: 166 °C Grade Count:13 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Fiberfil® J-60/30/E/HF Polypropylene Homopolymer, 30% Glass Reinforced, Chemically coupled, improved flow Information provided by FIBERFIL Engineered Plastics |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | |
MTI ThermoStran® PP-30G Long Glass Fiber Compound ThermoStran® is custom designed long fiber thermoplastic compound (LFC) engineered to meet specific end use requirements. Continuous fibers are pultruded to yield pellets with fibers equivalent t.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® POM CO GF15 CC 15% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 15% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 CC LE 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Chemically Coupled and Low ExtractablesInformation provided by TP Composites, .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® PP GF20 CC GL2 BK 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 20% Filler by WeightAdditive: Graphite Powder Lubricant(2%)Features: Chemically Coupled and LubricatedAppearance: BlackInf.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP VERTON MV00ES PP LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF20 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® PP GF50 CC HF BK 50% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 50% Filler by WeightFeatures: Chemically CoupledAppearance: BlackInformation provided by TP Composites, Inc... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | Unannealed; ASTM D648 |
Techmer ES Luriblend® POM CO AF15 Availability: North AmericaForms: PelletsAdditive: Aramid Resin Lubricant(15%)Features: Lubricated, Copolymer, Good Wear Resistance and Low FrictionInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | ASTM D648 |
Azdel Plus R401-B01 40% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R401-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Asahi Kasei Thermylene® P7-30FG-0890 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 309 °F | |
Reliance Industries Polypropylene - 40% Glass filled Information provided by Reliance Industries |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 °C | 310 °F | ASTM D648 |
Adell ER-17 Homopolymer Polypropylene, 30% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 154 - 279 °C | 309 - 534 °F | Average value: 208 °C Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |