Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Deflection Temperature at 1.8 MPa (264 psi) = 309 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 154 °C

@Thickness 6.35 mm
309 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne LubriOne™ AT-000/10T Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C

@Thickness 6.35 mm
309 °F

@Thickness 0.250 in
Unannealed; ASTM D648
PolyOne LubriOne™ AT-000/15T Acetal (POM) Copolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
Unannealed; ISO 75-2/A
PolyOne OnForce™ LFT PP-50LGF/001 UV Black Polypropylene Homopolymer (PP Homopolymer)
PolyOne's Long Fiber Thermoplastic (LFT) compounds are formulated for demanding applications which require high stiffness and good impact such as metal replacement or other structural applications. ..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
120°C/h; ISO 75/1
Polykemi AB POLYfill PPH GF3050 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Solvay Specialty Polymers Amodel® A-1240 HS Polyphthalamide (PPA) Resin, 40% Mineral Reinforced, Dry As Molded &nbs
AMODEL A-1240 polyphthalamide (PPA) resins are 40% mineral filled resins that have high deflection temperature, flexural modulus, and tensile strength. They mold with low warpage, have excellent di..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded  (
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ISO 75Af
Solvay Specialty Polymers Amodel® AP-9240 NL Polyphthalamide (PPA) Resin, 40% Mineral Filled, Dry as Molded  (
AMODEL AP-9240 NL resin is a 40% mineral-filled, impact-modified polyphthalamide (PPA). It was designed to provide a smooth molded surface suitable for many decorative applications. This resin offer..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
PolyOne Edgetek® NJ-10GF/000 Nylon 12 - 10% Glass Fiber  (discontinued **)
Data provided by PolyOne.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP VERTON MV00ES PP
LNP* VERTON* MV00ES is primarily a concentrate used for blending purposes. This is a 70% long glass fiber Polypropylene compound. Added features of this grade are: Heat Stabilized
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
Flatw 80*10*4 sp=64mm; ISO 75/Af
SABIC Innovative Plastics LNP THERMOTUF VF1001S Super Tough Nylon
LNP* Thermotuf* VF1001S is a Super Tough Nylon containing glass fiber. Characteristics of this grade is Heat Stabilized.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
GB-1634
Zhejiang Juner PA-A6-1 MF25%
Applications: Shell of Middle & Top Grade MCB, Pedestal & Shell of Low Voltage Electrical ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
0.125";; ASTM D648
Diamond Polymers NPP25-0504LGF40 40% Long Glass Fiber Filled Copolymer Polypropylene
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Adell ER-36 Homopolymer Polypropylene, 30% Glass Reinforced
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Chem Polymer Durlex 715 G PBT, 15% Glass Reinforced
A lubricated, 15% glass reinforced PBT offering a balance of rigidity, dimensional stability and toughness.Data provided by the manufacturer, Chem Polymer.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
A. Schulman ComAlloy Hiloy® 104 Polypropylene, Glass Reinforced
Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Asahi Kasei Thermylene® P7-30FG-0684 30% Glass Fiber Reinforced, Heat and UV Stabilized
Information provided by Asahi Thermofil
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
E-Polymers SEPAZ® LC30 PP Copolymer LFT Resin
Long Fiber Thermoplastics: SEPAZ LFT products, injection moldable long fiber-reinforced thermoplastics (LFT), are made using a unique pultrusion that thoroughly wets out the glass fibers and deliver..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
Reliance Industries Polypropylene - 40% Glass filled
Information provided by Reliance Industries
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ISO 75-2
Borealis Xmod™ GB306SAF Polypropylene, Glass Fiber Reinforced
Xmod™ GB306SAF is a 35 % chemically coupled high performance glass fiber reinforced polypropylene compound intended for injection molding. The product is available in standard black 9502. This mat..
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
PolyOne Edgetek® MP-30GF/000 Modified PPO - 30% Glass Fiber Reinforced  (discontinued **)
Data provided by PolyOne.
Deflection Temperature at 1.8 MPa (264 psi) 154 °C

@Thickness 6.40 mm
309 °F

@Thickness 0.252 in
unannealed; ASTM D648
SABIC Innovative Plastics NORYL PX2944 PPE+HIPS (Asia Pacific)
PPE/PS, GF20%, high heat, non-FR
Deflection Temperature at 1.8 MPa (264 psi) 154 °C
309 °F
ASTM D648
Adell ER-16 Homopolymer Polypropylene, 30% Glass Reinforced
Data provided by Adell Plastics, Inc.
Deflection Temperature at 1.8 MPa (264 psi) 154 - 279 °C
309 - 534 °F
Average value: 208 °C Grade Count:12
Overview of materials for Polyphthalamide (PPA), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o..