Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYblend 50LG PC/ABS-Blend, Low Gloss Information provided by Polykemi AB |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 3.20 mm |
221 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® CS9610 PC+ABS (Europe-Africa-Middle East) Cycoloy* CS9610 is a FR PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering optimum mechanical & impact balance and excellent flammability and low smoke behavior... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Cycoloy® XCY620 PC+ABS PC+ ABS Automotive applications, High Impact and High Flow, ductility at low temperature, excellent properties retention after Hydrolytic and Heat Aging |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ASTM D648 |
Gichem GIBLEND E45400 Polycarbonate / ABS
(discontinued **) Polycarbonate and ABS blend, high fluidity. Medium Injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.35 mm |
221 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
Covestro Bayblend® KU2-1500 Polycarbonate + ABS Blend, Extrusion/Blow-Molding
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | |
Lehmann & Voss LUVOCOM® 80-8444 Polyacetal-copolymer, unreinforced Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.dynamic stressReduced moment of inertia compared with metal parts.Isotropic shrinkage character.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
ASTM D648 |
Kingfa MAC-501 Modified PC/ABS Alloy Features:Excellent balance propertiesGood weather resistanceGood impact strengthGood processing propertiesSuit for electro-platingApplications:Injection moldingAutomobile license plateWater tank cov.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | not annealed; ASTM D648 |
Aardvark Polymers AARTEL® 2000 Rotational Molding Resin Aartel® 2000 POM is a premium homopolymer acetal for rotational molding applications. Aartel® 2000 offers high performance properties and is a high flow, fast cycling polymer.Information prov.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® SG3250 PBT+PET+MF25% Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical XR409HJ ABS, Heat Resistance, Curl Fit Feature: Injection Molding, Heat Resistance, Curl FitApplication: Automotives Interior & Exterior Housing (P/W Switch Housing Etc)CAS No. 25120-20-1, 9003-56-9 and 25747-74-7Information provided by .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ISO 75-1/-2 |
Mitsubishi Xantar® C CM 406 FD C CM 406 Polycarbonate/ABS Blend (European Grade) Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 3.20 mm |
221 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL PX6120 PPE+PS Noryl PX6120 is an unfilled material with good flow, high Impact and chemical resistance against cleaners. Noryl PX6120 is developed for personal care appplications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Unannealed; ASTM D648 |
Solvay Specialty Polymers Ryton® QC220N Polyphenylene Sulfide (PPS) Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® 1731A PBT+PC (Europe-Africa-Middle East) PBT+PC, Good Impact , Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® 1731J PBT+PC (Europe-Africa-Middle East) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Xenoy® EXXY0112 PBT+PC (Asia Pacific) PBT+PC, Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics Xenoy® X5410 PC+PET (Europe-Africa-Middle East) Mineral filled PC+PET resin with high heat dimensional stability for paint systems. It has very low CTE and excellent flow - impact balance for automotive exterior applications, like body panels, ta.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Flatw 80*10*4 sp=64mm; ISO 75/Af |
SABIC Innovative Plastics XYLEX X7507 PC+POLYESTER F-1 weathering certified in natural color, specially designed for Pool & Spa applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ISO 75-1/-2 |
Styrolution Luran® S KR 2864 C Colored ASA+PC Description: Easy flowing injection molding grade with heat resistance for parts with thin walls and/or with adverse flowpath/wall thickness ratios.Applications: Mobile phone housings.Information pr.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | Edgew 120*10*4 sp=100mm; ISO 75/Ae |
SABIC Innovative Plastics NORYL PX1185 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1185 is a special NORYL grade developed for extrusion of automotive trims. NORYL PX1185 offers high heat resistance and good impact performance. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | unannealed; ISO 75-A |
Styron Pulse® 920 MG PC/ABS An inherently matt medium heat, medium impact PC/ABS resin, PULSE™ 920 MG is designed for interior automotive applications where a matt aesthetic is required.Information provided by DowThis pro.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL CRX1005 PPE+HIPS (Asia Pacific) PPE+PS Chemical resistance improved |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ISO 75-1/-2 |
EMS-Grivory Grivory® GM-4H PA*-MD40 Product description: Grivory GM-4H natural is a 40 % mineral reinforced engineering thermoplastic material based on a combination of semi-crystalline Polyamide with partially aromatic copolyamide. G.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ISO 75-2 |
BASF Ultraform® Z2320 003 POM Description: Is a POM, rapidly solidifying grade for applications with exceptional demands on flowability.Information provided by BASF |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 - 115 °C | 221 - 239 °F | ASTM D648 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C @Thickness 6.40 mm |
221 °F @Thickness 0.252 in |
Method A; ASTM D648 |
Bhansali Engineering Abstron KU602M ABS Heat Resistant High rigidityInformation provided by Bhansali |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 105 °C | 221 °F | ASTM D648 |
Samyang Triloy® 200N PC/ABS alloy, Flame Retardant Characteristics:Impact resistantFlame retardantApplications:Cellular phoneMonitor housingCoffee makerHair dryerO/A partAll information provided by Samyang |