Material Notes:
Ryton® PPS Fiber Grade Resins are high molecular weight polyphenylene sulfide polymers suitable for monofilament and/or multifilament fiber extrusion. They exhibit excellent thermal stability and chemical resistance.Features: Good Chemical Resistance; Good Thermal Stability; High Molecular WeightAdditional Properties: Ash Content - ISO 3451-1 0.3 wt%; Color L - 90.0; Volatiles - (150°C): < 0.3 wt%; Weight Loss on Heating - (300°C): < 0.50 wt%Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.35 g/cc
0.0488 lb/in³
ASTM D792
Water Absorption at Saturation 0.050 %
0.050 %
ASTM D570
Melt Flow 170 g/10 min

@Load 5.00 kg,
Temperature 316 °C
170 g/10 min

@Load 11.0 lb,
Temperature 601 °F
Procedure B; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 85.0 MPa
12300 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 50.0 µm/m-°C

@Temperature -50.0 - 50.0 °C
27.8 µin/in-°F

@Temperature -58.0 - 122 °F
1
Melting Point 285 °C
545 °F
ISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 105 °C
221 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.2

@Frequency 1.00e+6 Hz
3.2

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 24.0 kV/mm
610 kV/in
ASTM D149
Dissipation Factor 0.0020

@Frequency 1.00e+6 Hz
0.0020

@Frequency 1.00e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Availability Asia Pacific
Europe
Latin America
North America
Form Pellets
Processing Technique Filament Extrusion
RoHS Compliance RoHS Compliant