Deflection Temperature at 8.0 MPa 80.0 - 110 °C
176 - 230 °F
ISO 75-C
Raschig Group AMPLA® 2000 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Low post-shrinkage, very good electrical values, high heat resistance, very good sliding behavior, ve..
Deflection Temperature at 8.0 MPa 80.0 - 110 °C
176 - 230 °F
Injection; ISO 75-C
Raschig Group AMPLA® 2500 melamine-modified polyester
Halogen-free, organically and inorganically filled melamine-modified Polyester molding compound. Excellent elasticity and shock resistance, low post-shrinkage, very good electrical values, high heat..
Deflection Temperature at 8.0 MPa 80.0 - 110 °C
176 - 230 °F
Injection; ISO 75-C
Raschig Group AMPLA® 7250 melamine-modified polyester
Cellulose reinforced melamine-modified Polyester molding compound. Very good electrical values, excellent heat resistance, excellent surface quality, low post shrinkage. This product meets the allow..
Deflection Temperature at 8.0 MPa 80.0 - 100 °C
176 - 212 °F
Injection; ISO 75-C
Raschig Group AMPLA® 7500 melamine-modified polyester
Organically and inorganically filled melamine modified Polyester molding compound. Low post-shrinkage, very good electrical values, excellent heat resistance, very good sliding behavior and wear sta..
Deflection Temperature at 8.0 MPa 80.0 - 120 °C
176 - 248 °F
ISO 75-C
Raschig Group RALUPOL® 2100 UP Polyester
Organically and inorganically filled polyester molding compound. Low post-shrinkage, very good electrical values, good mechanical strength. This product meets the allowed upper limits for heavy meta..
Deflection Temperature at 8.0 MPa 80.0 - 110 °C
176 - 230 °F
Average value: 86.0 °C Grade Count:5
Overview of materials for Nylon 12, 20% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. ..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Lanxess Durethan® AKV 325 H2.0 901510 Nylon 66, 25% Glass Fiber
PA 66, 25% glass fibers, extrusion- and blow molding grade, branched, high viscosity, good heat-ageing resistance, good hydrolysis resistance
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Lanxess Durethan® BKV 130 GIT 900116 Copolyamide, 30% Glass Fiber
CoPA, injection molding grade, 30% glass fibers, elastomer-modified, suitable for GIT (gas assisted technology), good surface finishApplication Examples: Chain-saw handles, office chair armrests, of..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral
PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Lanxess Durethan® BKV 30 G H2.0 900051 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance, good UV s..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
Lanxess Durethan® BKV 30 G H2.0 900116 Nylon 6, 30% Glass Fiber
PA 6, injection molding grade, 30% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 30 H2.0, heat-stabilized, good heat-ageing resistance
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1,-2
Lanxess Durethan® BKV 325 Z H2.0 901510 Nylon 6, 25% Glass Fibers
PA 6, 25% glass fibers, blow molding, impact modified, heat-ageing stabilized
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® AG-25 HM PA66-GF25
Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important pro..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-15H nat PA12-GF15
Product description: Grilamid LV-15H is a 15% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptiongood dimension..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-23 ESD PA12-GF23
Product description: Grilamid LV-23 ESD is a 20% fiber reinforced, anti-static injection molding grade Polyamide 12 (PA12). Grilamid LV-23 ESD is heat stabilized, is easy to process and demold. The ..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-23H PA12-GF23
Product description: Grilamid LV-23H is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile. Good chemical resistanceGood UV stabili..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® LV-2H PA12-GF20
Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona..
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSG-15/4 PA666-GF15
Information provided by EMS Grivory
Deflection Temperature at 8.0 MPa 80.0 °C
176 °F
ISO 75-1/-2
EMS-Grivory Grivory® TSGK-30 X PA666-(GF+GB)30
Product description: Grilon TSGK-30 X is a heat stabilized PA66 + PA6 injection molding grade with a 30% reinforcement combination (glass fibers and glass beads). Grilon TSGK-30 X has the following ..
Copyright © lookpolymers.com All Rights Reserved