Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1330 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1330 polycarbonate (PC) siloxane copolymer resin is a UV stabilized opaque injection molding (IM) and sheet extrusion grade. This resin offers extreme low temperature (-60 C) ductility in .. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® FXD9810 PC Copolymer (Europe-Africa-Middle East) Non-chlorinated, non-brominated Flame retardant PC-siloxane copolymer blend. Excellent processability, super high flow, good impact, UL rated V-0. Limited translucent colors.This data was supplied b.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 18 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 22 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® 25 SR FD Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G4F 23 R Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G4F 25 UR Polycarbonate-20% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
IEC 60695-2-12 |
Styron CALIBREâ„¢ 303-10 Polycarbonate Resin Overview: CALIBREâ„¢ 300-10 polycarbonate resins offer exceptional impact resistance, heat distortion resistance and optical clarity as well as high melt strength for blow molding and sheet appli.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2400 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2407 MAS070 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 875 °C @Thickness 1.00 mm |
1610 °F @Thickness 0.0394 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2667 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Med.. |
|||
Glow Wire Test | 875 °C @Thickness 0.750 mm |
1610 °F @Thickness 0.0295 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 875 °C @Thickness 0.750 mm |
1610 °F @Thickness 0.0295 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 875 °C @Thickness 0.750 mm |
1610 °F @Thickness 0.0295 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
Ignitability; IEC 60695-2-13 |
Eurostar Starflam BFR460B1 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR460B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Glow Wire Test | 875 °C @Thickness 0.750 mm |
1610 °F @Thickness 0.0295 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecopet® PT70 KK45 PET, 45% glass fiber/mineral reinforced, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecotek® PC43 GR003 TD70 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, light grey Information provided by Eurotec® |
|||
Glow Wire Test | 875 °C @Thickness 0.400 mm |
1610 °F @Thickness 0.0157 in |
Ignition Temperature; IEC 60695-2-13 |
Ascend Performance Materials Vydyne® ECO315 BK06 Nylon 66/6, Flame Retardant, DAM Vydyne® ECO315 BK06 is a non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent toughness and ductility. It is lubricated for machine feed and easy mold release and has Underwri.. |
|||
Glow Wire Test | 875 °C @Thickness 0.380 mm |
1610 °F @Thickness 0.0150 in |
Ignition Temp; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® ECO-315 Nylon 66/6, non-halogenated, ignition resistant, DAM Vydyne® ECO315 is non-halogenated, unfilled, flame-retardant PA66/6 copolymer with excellent strength and toughness. It is lubricated for machine feed and has an Underwriters Laboratories UL 94 fla.. |
|||
Glow Wire Test | 875 °C @Thickness 3.00 mm |
1610 °F @Thickness 0.118 in |
GWIT; IEC 60695-2-13 |
Covestro Makrolon® LED2643 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• LED lighting, optics, .. |
|||
Glow Wire Test | 875 °C @Thickness 2.00 mm |
1610 °F @Thickness 0.0787 in |
GWIT; IEC 60695 |
Eurotec® Tecolen® CP30 NL XA80 PPCP, flame retardant - halogen (RoHS compliant), heat stabilized, natural Information provided by Eurotec® |
|||
Glow Wire Test | 875 °C @Thickness 1.50 mm |
1610 °F @Thickness 0.0591 in |
Flammability Index; IEC 60695-2-12 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Glow Wire Test | 875 °C @Thickness 0.400 mm |
1610 °F @Thickness 0.0157 in |
GWIT; IEC 60695-2-13 |
Lanxess Durethan® AKV 25 F30 000000 Nylon 66, 25% Glass Fiber PA 66, 25% glass fiber, injection molding, flame retardantInformation provided by LANXESS. |