Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid B3N Unfilled, Nucleated PA6 Description: Nilamid B3N is an unfilled, nucleated NYLON 6. It is fast cycling, and combines ease of processing with good overall mechanical characteristics.Key characteristics: Fast cyclingEasy pro.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 2014R PC (Europe-Africa-Middle East) LEXAN 2014R is a medium viscosity flame retardant grade, This material contains a release agent to ensure easy processing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region... |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® 920 PC (Europe-Africa-Middle East) LEXAN 920 is a low viscosity flame retardant grade, especially suitable for electrical applications. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1192T PC Copolymer Lexan* EXL1192T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade with extra release properties for food contact applications. This resin offers good low temp.. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1464T PC Copolymer Lexan* EXL1464T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers extreme low temperature (-40 °C) ductility in combination with medium flo.. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Flammability Index; IEC 694-2-12 |
Nilit Nilamid A3 N H2 Nucleated, Heat Stabilized Nylon 66 Description: Nilamid A3 N H2 is a nucleated, heat stabilized NYLON 66 with excellent flow characteristics and very fast cycle time. It is widely used throughout many industries for mass production a.. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1112T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with high flow char.. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Lexan® EXL1860T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1860T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers improved release performance, cold temperature (0 °C) ductility in combi.. |
|||
Glow Wire Test | 850 °C @Thickness 1.60 - 6.00 mm |
1560 °F @Thickness 0.0630 - 0.236 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU)
(Unverified Data**) Udel P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand prolonged e.. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® F 23 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® FC 19 R Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® G8F 23 UR Polycarbonate-40% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® MX 1081 Polycarbonate-10% Glass Reinforced Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances .. |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignitability Temperature; IEC 60695-2-13 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Flammability Index, IEC 60695-2-12 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Glow Wire Test | 850 °C @Thickness 1.60 - 6.00 mm |
1560 °F @Thickness 0.0630 - 0.236 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Solvay Specialty Polymers Udel® P-1700 Polysulfone (PSU) Udel® P-1700 polysulfone (PSU) is a tough, rigid, high-strength thermoplastics suitable for continuous use up to 300°F (149°C). It is resistant to oxidation and hydrolysis and withstand pro.. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 850 °C @Thickness 0.750 mm |
1560 °F @Thickness 0.0295 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2407 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glow Wire Test | 850 °C @Thickness 1.00 mm |
1560 °F @Thickness 0.0394 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2600 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2607 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2805 MAS145 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 2805 MAS152 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Med.. |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm |
1560 °F @Thickness 0.0787 in |
GWFI; IEC 60695-2-12 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 850 °C @Thickness 1.50 mm |
1560 °F @Thickness 0.0591 in |
b.o. EDF HN60 E.02 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glow Wire Test | 850 °C @Thickness 0.800 mm |
1560 °F @Thickness 0.0315 in |
Glow Wire Ignition Temperature, dry; IEC 60695-2-13 |
DSM EcoPaXX® Q150-D PA410 Low/Medium Viscosity |
|||
Glow Wire Test | 850 °C @Thickness 2.00 mm |
1560 °F @Thickness 0.0787 in |
GWFI; IEC 60695 |
Eurotec® Tecotek® PC43 GR10 BK002 PC, 10% glass fiber reinforced, black Information provided by Eurotec® |
|||
Glow Wire Test | 850 °C @Thickness 3.00 mm |
1560 °F @Thickness 0.118 in |
Glow Wire Ignition Temperature; IEC 60695-2-13 |
Mitsubishi Xantar® F 22 UR Polycarbonate Xantar® materials are engineered for performance, consistency and reliability. This makes Xantar® resins ideal for interior automotive components, electrical equipment and consumer appliances wher.. |
|||
Glow Wire Test | 850 °C @Thickness 2.50 mm |
1560 °F @Thickness 0.0984 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |