Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Sheet/Thermoforming Grade
Manufacturer LyondellBasell (former Equistar)
Trade Name Petrothene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Petrothene® LP500210 High Density Polyethylene (Sheet & Profile Grade).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
ApplicationsThe PETROTHENE LP 5002 series of polyethylene resins exhibits excellent environmental stress crack resistance.Regulatory StatusThe LP 5002 base resin meets the requirements of Food and Drug Administration regulation, 21 CFR 177.1520. This regulation allows the use of this olefin polymer in "articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply. Contact your Equistar sales representative for more information. Processing TechniquesSpecific recommendations for processing LP 5002 can only be made when the processing conditions, equipment and end use are known. For further suggestions, please contact your Equistar sales representative.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ASTM D1505
Environmental Stress Crack Resistance >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D1693
ESCR, Bottle >= 1000 hour
>= 1000 hour
F<sub>50</sub>; ASTM D2561
Melt Flow 0.20 g/10 min
0.20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.965 GPa
140 ksi
ASTM D790
Tensile Impact 131 J/cm
245 ft-lb/in
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 66.0 °C
151 °F
ASTM D648
Vicat Softening Point 122 °C
252 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
F<sub>50</sub>; ASTM D746
Descriptive Properties Value Comments
Antistat High