Dow Engage® 8180 Polyolefin Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Dow Chemical
Trade Name Engage®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Engage® 8180 Polyolefin Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Engage® 8180 polyolefin elastomer is a lower density, high performance ethylene-octene copolymer that has excellent flow characteristics and provides good impact properties in blends with polypropylene (PP) and polyethylene (PE). It is widely used in TPO applications where excellent flow temperature impact properties are desired. Engage® 8180 also provides high filler loading capability and excellent electrical properties. When cross-linked by peroxide, silane, or irradiation, it gives exceptional heat aging, compression set, and weather resistance properties. The product form is free-flowing pellets.Information provided by manufacturer.This former DuPont Dow Elastomers product line is now produced by Dow Chemical.
Physical Properties Metric English Comments
Density 0.863 g/cc
0.0312 lb/in³
ASTM D792
Mooney Viscosity 35

@Temperature 121 °C
35

@Temperature 250 °F
ML 1 + 4; ASTM D1646
Melt Index of Compound 0.50 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
ASTM D2240
Hardness, Shore D 16
16
ASTM D2240
Tensile Strength, Ultimate 8.80 MPa
1280 psi
508 mm/min; ASTM D638
Tensile Strength, Yield 1.70 MPa
247 psi
508 mm/min; ASTM D638
Elongation at Break 860 %
860 %
508 mm/min; ASTM D638
2% Secant Modulus 0.00830 GPa
1.20 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 49.0 °C
120 °F
DSC, 10°C/min; DuPont Test
Vicat Softening Point 38.0 °C
100 °F
ASTM D1525
Brittleness Temperature <= -76.0 °C
<= -105 °F
ASTM D746
Descriptive Properties Value Comments
Comonomer Content 42 wt%
Dow Method (<sup>13</sup>C NMR/FTIR)