Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glow Wire Test | 750 °C | 1380 °F | STN IEC 60695-2-10 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Glow Wire Test | 750 °C | 1380 °F | |
Plastcom SLOVASTER® B1 GF 45 PBT, 45% glass fibre FeaturesPBT for injection moulding, chemically reinforced with 45% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYblend 85FS GF10 PC/ABS-Blend, Glass Fiber reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PP CQX10030 R3 Polypropylene, Mineral Reinforced, Scratch Resistant Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PP HIP15025 HC Polypropylene Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPC T4020 H Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF15020 PD1 NBR PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF5030 HC Polypropylene Homopolymer, Glass Fibre-Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH T8038 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYlux 3709MLB PC/PBT-Blend, Paintable Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 0.750 mm |
1380 °F @Thickness 0.0295 in |
IEC 60695-2-12 |
SABIC Innovative Plastics Lexan® LUX2114G PC (Europe-Africa-Middle East) Lexan LUX2114G (EXRL0943) is a diffusive, mid viscosity, uv stabilized, flame retardant polycarbonate with improved light transmission and providing good colorstability under heat exposure. Develope.. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-13 |
SABIC Innovative Plastics LNP KONDUIT PX11313 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compounding |
|||
Glow Wire Test | 750 °C | 1380 °F | |
Plastcom SLOVASTER® B GB 20 M PBT, 20% glass beads FeaturesPBT for injection moulding, chemically reinforced with 20% glass fibre. Characterised by excellent properties also at minus temperatures like eg. modulus of elasticity in tension and bending.. |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PP EVR8025H UV Polypropylene/EDPM, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPC T25020 UV Polypropylene Copolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF3030 PD2 PP, Glass Fiber-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH Q15030 E10 Polypropylene Homopolymer, Mineral Reinforced, Elastomer Modified Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYshine PBT D201 GF20 PBT, Glass Fiber Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 3.20 mm |
1380 °F @Thickness 0.126 in |
Glow Wire Flammability Index; IEC 60695-2-12 |
SABIC Innovative Plastics Geloy CR7520 ASA (Europe-Africa-Middle East) Geloy CR7520 is a general purpose injection moulding grade, blend of ASA/SAN. It can be positioned for outside parts in various markets, such as telecommunication, transportation, B&C, lighting and .. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-12 |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-12 |
Menzolit Menzolit® BMC 3000 Unsaturated Polyester UP BMC 3000 is a special BMC suitable for the use in microwave and cookware applications.It has high temperature resistance, and meets requirements for food contact applications. It has a high gloss fi.. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCA105 PPE-TPE (Europe-Africa-Middle East) Flexible, non-halogenated FR mPPE extrusion grade ideal for evaluation in applications such as wire insulation. Flame retardant performance capable of meeting VW1 and 105C temperature rating requir.. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCD801AU PPE-TPE (Asia Pacific) Flexible, UV stabilized, halogen free extrusion grade for applications such as wire insulation and cable jacket. Good color stability after UV weathering per ASTM D4459. Light color capable. Flame r.. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-13 |
SABIC Innovative Plastics NORYL WCD835 PPE-TPE Flexible, low odor, halogen free extrusion grade intended for evaluation in applications such as wire insulation and cable jacket. Flame performance capable of meeting UL VW1 requirements. 80C end.. |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH GF8020 PB Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH T5060 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C @Thickness 2.00 mm |
1380 °F @Thickness 0.0787 in |
IEC 695-2-1 |
Polykemi AB POLYfill PPH TS15030 D Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
Glow Wire Test | 750 °C | 1380 °F | |
Polyram RamSter PF391G6 PBT, 30% Glass Fiber 30% glass-fiber reinforced, surface modified PBT for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Glow Wire Test | 750 °C | 1380 °F | IEC 60695-2-12 |
Sax Polymers SAXATEC 4210 Acrylonitrile Styrene Acrylate SAXATEC 4210 is a high heat resistant, high viscosity and weatherable ASA injection molding grade, characterized by high impact strength and high stiffness.Information provided by SAX Polymers |
|||
Glow Wire Test | 750 °C | 1380 °F | CEI 60695/2/1 |
Addiplast Addilene PMD 50265 Flame Retardant Polypropylene Flame retardant, high rigidityInformation provided by Addiplast. |