Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics LNP KONDUIT PX10322 PA 6 (Asia Pacific) Thermally conductive mineral filled PA6 FR compound, with through-plane and in-plane thermal conductivity of 1.7 W/(m*K) and 4.7 W/(m*K) respectively, conforming to ASTM E 1461 test standard. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 1.50 mm |
284 °F @Thickness 0.0591 in |
UL746B |
Covestro Apec® DP9-9354 High-Heat Polycarbonate, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 315 PBT (Asia Pacific) General purpose polyester. Fully imported product from USA |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 325 PBT General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 325 PBT (Asia Pacific) General purpose, unreinforced, improved processing. Applications like sprinklers and nozzles, pumps, door handle, tank covers, pens, pencils etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 357 PBT+PC PC/PBT, Unreinforced, impact modified, UL94V-0 rated. Applications like bobbins, switches and enclosures. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 357U PBT (Asia Pacific) Unreinforced PBTP, UL94 V-0/5VA rated. Improved UV resistant version of VALOX 357. Nonblooming flame retardant. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 457 PBT (Asia Pacific) 6.5% GR PBT, UL94 V-0/5V. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 771 PBT 35% mineral/glass reinforced flame retardant grade with a CTI performance level class of 0 rating. Applications which may see electrical arcing. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 780 PBT (Asia Pacific) 40% gl/min, UL94 V-0 rated. Nonblooming flame retardant. Circuit breaker handles/housings, motor coil housings. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® DR48 - CS1049 PBT (Europe-Africa-Middle East) VALOX DR48 is a 15 % glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromot.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® DR48 PBT (Asia Pacific) 17% glass reinforced, flame retardant grade UL-94 rated V-0/5VA. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® DR51 PBT 15% GR polyester, excellent mechanical, thermal and electrical performance. Non-flame retardant. Spotlights, appliance housings, handles, connectors |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357 PBT+PC Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357 PBT+PC (Asia Pacific) Valox* Resin IQ357: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357U PBT+PC Valox* Resin IQ357U: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified and UV stabilized resin. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Asia Pacific) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ420 PBT (Europe-Africa-Middle East) Environmentally responsible Valox iQ420 resin: iQ-PBT+ 30% glass fiber reinforcement. Targeted for use in electrical motors, connectors, pump housings, spotlights, appliance handles, etc. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 430 PBT (Europe-Africa-Middle East) VALOX 430 is 33% glass reinforced, impact modified PBT injection moulding resin. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® 451E PBT 20% GR. Easy flow version of VALOX 451. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® ENH3500 PBT (Europe-Africa-Middle East) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® IQ357M PBT+PC (Europe-Africa-Middle East) Valox* Resin IQ357M: Environmentally responsible, low carbon footprint iQ* PBT + PC alloy. UL94 V-0 @0.63 mm. Impact modified, easy flow product with mold release. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
SABIC Innovative Plastics Valox® V3504 PBT (Asia Pacific) VALOX EXVX0197 is an unreinforced, flame retardant PBT injection moulding resin. Applications: electrical industry, bobbins, keyboard, switches and switch components and appliance housings. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
Covestro Apec® 1797 High-Heat Polycarbonate This linear, amorphous copolycarbonate is most suitable for applications that must withstand high temperatures and exhibit toughness, impact resistance and high transparency. These properties, along.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | |
Covestro Petlon® 3530 Semi-Crystalline PET, 30% Glass Fiber
(discontinued **) Characteristics: Excellent Electrical Properties, High Heat and Chemical ResistanceApplications: Automotive (Underhood), Appliances, Casings and HousingsProcessing: Injection Molding (Melt Temperatu.. |
|||
UL RTI, Mechanical without Impact | 140 °C | 284 °F | UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 2.00 mm |
284 °F @Thickness 0.0787 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |
|||
UL RTI, Mechanical without Impact | 140 °C @Thickness 6.00 mm |
284 °F @Thickness 0.236 in |
UL 746B |
DuPont Performance Polymers Rynite® 530 BK503 PET
(Unverified Data**) Rynite® 530 BK503 is a 30% glass reinforced modified polyethylene terephthalate with outstanding balance of strength, stiffness, and toughness, excellent electrical properties, surface appearance, .. |