Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CY6414 PC (Europe-Africa-Middle East) Flame retardant modified PC blend using non-brominated and non-chlorinated flame retardant systems, offering high heat for application in appliances, lighting and electrical market. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 123 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 123 PC (Asia Pacific) Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 153 PC (Asia Pacific) Nonhalogenated. 2.5 MFR. Blowmolding/extrusion. UV-stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 191 PC (Asia Pacific) Nonhalogenated. 8.5 MFR. High impact. Thick wall sections. Opaques only. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 223 PC 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 223 PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. UV stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 223R PC 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 223R PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® 223S PC (Asia Pacific) 17.5 MFR, for small, intricate parts. Improved flame retardance. Internal mold release. UV stabilized. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® LS1 PC (Asia Pacific) Automotive lens applications. Low viscosity. UV-stabilized. Transparent colors only. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® LS2 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® LS2 PC (Asia Pacific) Automotive lens applications. Medium viscosity. UV-stabilized. Transparent colors only. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® LS3 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Automotive lens applications. Medium-high viscosity. UV-stabilized. Adhesion to coatings. Transparent colors only. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Asia Pacific) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6411 PC Copolymer (Europe-Africa-Middle East) Lexan* ML6411 polycarbonate (PC) siloxane resin, is a high flow opaque injection molding (IM) grade with very low temperature ductility characteristics. This grade offers UL94 V0 @ 1.5mm and 5VA @ 3.. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6412 PC Copolymer (Asia Pacific) ML6412 is an impact modified PC resin with non-brominated, non-chlorinated flame retardant system. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6413 PC Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6413 PC (Asia Pacific) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML6413 PC (Europe-Africa-Middle East) Lexan* ML6413 resin is an impact modified, flame retardant polycarbonate grade with Br- & Cl-free FR systems. It features improved light shielding capability with good flow, impact and thermal prope.. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1130 PC (Asia Pacific) UV-stabilized. Good clarity, heat resistance, property retention and dimensional stability. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC LNP* Lubricomp* Lexan_WR2210 compound is an alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_WR2210 PC (Asia Pacific) Alternative polymeric wear additive technology. No silicones, superior processability/part appearance. Flow similar to LEXAN 121. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Valox® 3706 PBT+PC Impact modified PBT+PC resin. Outdoor enclosure. Not available in all colors. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Noryl HS1000X PPE+PS PPE+PS blend. 13% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL 746C f1. Radiant Panel listing. Dielectric strength. Dimensional stability. Suitable for .. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | |
Eurostar Starflam PX06004 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX06004 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | |
Eurostar Starflam BFR200Y PA6, Flame Retardant, Injection Molded Starflam BFR200Y is Unfilled, Halogen Free and Red Phosphorous Free, Flame Retardant Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
UL RTI, Mechanical without Impact | 100 °C | 212 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® CH6410 PC+ABS (Europe-Africa-Middle East) CH6410 is a high heat, impact modified PC resin, with nonbrominated, nonchlorinated flame retardant system. Limited colors only.This data was supplied by SABIC-IP for the Europe-Africa-Middle East r.. |