Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200 PC+ABS (Asia Pacific) PC+ABS, excellent impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1200HF PC+ABS PC+ABS, excellent flow/impact/high heat resistance. Low temperature ductility. For automotive, appliance and electrical components. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® HC1204HF PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering good flow and excellent impact. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® EM2212 PC Automotive interiors. 10% glass-reinforced. Increased stiffness/structural ridigity. High modulus/ductile. Foamed skin instrument panel uses also. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® EM3110 PC (Asia Pacific) Automotive interiors. Optimizes flow/processability for cost effective thinner wall design uses. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HF1130R PC (Europe-Africa-Middle East) LEXAN HF1130R is a high flow, UV stabilized, grade especially designed for applications that require thin wall sections and higher flow lengths. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HFD4211 PC (Asia Pacific) Lexan* HFD4211 is a 10% glass filled, injection moldable grade designed for high flow and superior surface appearance. Internal mold release. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® HP9NR PC Low flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. For blow molding .. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Cycoloy® FXC810SK PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810SK is a multi purpose PC+ABS injection moulding grade, providing a favourable balance of engineering properties. CYCOLOY FXC810SK is suitable for those applications that require sparkl.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® 3412HF PC 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® BFL2000U PC Lexan* BFL2000U Polycarbonat (PC) resin is an injection moldable grade. It contains non-brominated, non-chlorinated flame retardant systems with UL-94 V0 rating. Lexan* BFL2000U is designed for hig.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL405 PC Various weight reductions at 0.250"" (6.38 mm) wall. Impact resistant, superior processing, excellent surface. UL94 V-0 at 0.120 |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® FL900S PC (Europe-Africa-Middle East) Foamable Lexan* FL900S polycarbonate resin is an ideal choice for structural components where load bearing capability at elevated temperature is a key requirement. It exhibits outstanding inpact str.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3729 PC (Europe-Africa-Middle East) LEXAN ML3729 is an UV stabilized grade, with an excellent flow. It contains a release agent to ensure easy processing. |
|||
UL RTI, Mechanical with Impact | 80.0 - 130 °C | 176 - 266 °F | Average value: 103 °C Grade Count:13 |
Overview of materials for Polycarbonate, 30% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
|
Covestro Makrolon® DP1-1243 Polycarbonate, Extrusion
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness >=0.700 mm |
176 °F @Thickness >=0.0276 in |
|
LG Chemical LUPOY SC1004AU PC, High Impact Description: Injection Molding, PC, High Impact, High Flow, Good WeatherabilityApplication: Electric & Electronic HousingCAS: 103598-77-2 and 143106-82-5Information provided by LG Chemical |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics NORYL SE100HX PPE+PS Improved productivity and reliability. Nonchlorinated, nonbrominated FR. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics LNP LUBRICOMP Lexan_LF1520A PC (Asia Pacific) 20% glass reinforced/15% PTFE filled PC. Flame retardant and wear resistant. Tight tolerances. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LN-1010RM High Light Reflection, Flame Resistant Polycarbonate Resin Polycarbonate-resin-base flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even at a thinner th.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.47 mm |
176 °F @Thickness 0.0579 in |
UL 746B |
Teijin Panlite® LN-3000RM High Light Reflection, Halogen-Free Flame Resistant Polycarbonate Resin Polycarbonate-resin-based halogen-free flame retardant and good light-reflection grade. It exhibits high light-reflection (over 96 %) at whole visible light range and also good light shut-out even a.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Noryl N190HX PPE+PS High gloss. 182F (83C) HDT. UL94 V-0/5VA rated.This data was supplied by SABIC-IP for the Americas region. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 1002 Description: Injection Molding Grade, Extra High GlossInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 2512 Description: Injection Molding Grade, Medium Impact, High FlowInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical with Impact | 80.0 °C @Thickness 1.50 mm |
176 °F @Thickness 0.0591 in |
UL 746B |
Diamond Polymers ABS 3502ELG Description: Injection Molding Grade, Medium Impact, Low GlossInformation provided by Diamond Polymers, Inc. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
Covestro Makrolon® ET3127 Polycarbonate Makrolon® polycarbonate resinMain characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characterist.. |
|||
UL RTI, Mechanical with Impact | 80.0 °C | 176 °F | UL 746B |
SABIC Innovative Plastics Lexan® ML3260 PC (Europe-Africa-Middle East) LEXAN ML3260 is a medium viscosity, 15% glass reinforced, flame retardant grade especially designed for applications like computer cartridges. |