Thermal Properties | Metric | English | Comments |
---|---|---|---|
UL RTI, Electrical | 160 °C | 320 °F | UL 746 |
Solvay Specialty Polymers Mindel® B-322 Polysulfone, Modified (PSU, Modified)
(discontinued **) Mindel B-322 is a glass filled, modified polysulfone developed specifically for molded electrical connector applications requiring excellent dimensional stability and resistance to warpage. This mat.. |
|||
UL RTI, Electrical | 160 °C | 320 °F | |
Haysite Ultratrac® H950 Glass Reinforced Polyester Sheet, Electrical Grade (GPO3) This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and t.. |
|||
UL RTI, Electrical | 160 °C | 320 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5001 PEI Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
UL RTI, Electrical | 160 °C | 320 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5001 PEI (Asia Pacific) Transparent, Standard flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
UL RTI, Electrical | 160 °C | 320 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5011 PEI Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
UL RTI, Electrical | 160 °C | 320 °F | UL 746B |
SABIC Innovative Plastics ULTEM CRS5011 PEI (Asia Pacific) Transparent, Enhanced flow Polyetherimide copolymer (Tg 225C) with enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO conforming, UL94 V0 listing. |
|||
UL RTI, Electrical | 160 °C | 320 °F | |
DuPont Teijin Films Teonex® Q51 Polyester Film, 48 Gauge Teonex® Q51 is biaxially oriented polyethylene naphthalate (PEN) film. It is slightly hazy with excellent handling properties for general purpose. It is commercially available in nominal 48 - 1000 .. |
|||
UL RTI, Electrical | 160 °C | 320 °F | |
DuPont Teijin Films Teonex® Q72 Polyester Film, 14 Gauge Teonex® Q72 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film. This ultra thin film which was developed for capacitor applications. It is commercially available in nominal 14.. |
|||
UL RTI, Electrical | 160 °C | 320 °F | |
DuPont Teijin Films Teonex® Q83 Polyester Film, 200 Gauge Teonex® Q83 is biaxially oriented, slightly hazy polyethylene naphthalate (PEN) film with excellent handling properties and high dimensional stability. It is commercially available in 100, 200 and .. |
|||
UL RTI, Electrical | 160 °C | 320 °F | 50% decrease of tensile strength after 20000h; 746B |
BASF Ultrason S 2010 G4 20% Glass Filled PSU Ultrason S 2010 G4 is a 20% glass reinforced, medium viscosity injection molding PSU grade with high rigidity and strength. |
|||
UL RTI, Electrical | 160 °C | 320 °F | |
Bulk Molding Compounds BMC 1412 Flame and Track Resistant BMC 1412 is an extremely versatile material. Flame and track resistant, low shrink for close dimensional control and surface smoothness, high physical properties. Developed for injection molding, bu.. |