Material Notes:
Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Environmental Stress Crack Resistance 500 hour

@Thickness 3.17 mm,
Temperature -40.0 °C
500 hour

@Thickness 0.125 in,
Temperature -40.0 °F
10% Igepal; ASTM D1693
>= 1000 hour

@Thickness 3.17 mm,
Temperature -40.0 °C
>= 1000 hour

@Thickness 0.125 in,
Temperature -40.0 °F
100% lgepal; ASTM D1693
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 21.4 MPa
3100 psi
ASTM D638
Elongation at Yield 11 %
11 %
ASTM D638
Flexural Modulus 0.827 GPa
120 ksi
ASTM D790
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 62.0 °C
144 °F