Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Unannealed; ISO 75-2/B |
PolyOne Bergamid™ A700 TM-YF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP COLORCOMP R1000 PA 66 LNP* COLORCOMP* R1000 is an unfilled Nylon 66. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/-2 |
DSM Akulon® S223-TP4 (Dry) Impact Modified Nylon 66 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 103FHS BKB038 Nylon 66
(Unverified Data**) Zytel® 103FHS BKB038 is a heat stabilized, lubricated, PA 66 resin for fast cycling.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 6.40 mm |
392 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® SG3250A PBT+PET+MF25% Description: Injection Molding, PBT+PET+MF25%, Good SurfaceApplication: Automotive (Head Lamp Bezel)CAS No. 24968-12-5, 25038-59-9 and 14807-96-6Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 6.40 mm |
392 °F @Thickness 0.252 in |
Unannealed; ASTM D648 |
LG Chemical Lupox® SG5150 PBT+PET+GF15% Description: Injection Molding, PBT+PET+GF15%, Good SurfaceApplication: E&E, Automotive (Door Latch)CAS No. 65997-17-3, 25038-59-9 and 24968-12-5Information provided by LG Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D1525, HDT Method B |
Loxim 330 01HB Nylon 6 Information provided by Loxim Industries |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | |
LATI Kelon® B FR H2 CE/25-V2HF PA 6, Mineral Reinforced, Flame Retardant, Heat Stabilized Polyamide 6 (PA6) based compound. Heat stabilized. Mineral filler. UL94 V-2 classified, halogens-based flame retardants and red phosphorous free.Availability: Africa & Middle East; Asia Pacific; Eur.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Ultem 1010X PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with low ionic contamination of less than 0.1 ppm each of leachable chloride and sulphates. ECO Conforming. Factory Mutual FM4910 compliant in recognized color.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics ULTEM PW1000 PEI (Europe-Africa-Middle East) Unfilled Standard flow Polyetherimide (Tg 217°C). Specific grade-colors aredesigned and certified for use in Potable Water applications. KTW, WRAS, ACS, NSF-61 and W270 certified. US FDA and Euro.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C @Thickness 3.20 mm |
392 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL GTX GTX986 PPE+PA66 (Europe-Africa-Middle East) Conductive GTX, CTE 6 |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/-2 |
DSM Akulon® K225-KWS (Dry) Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6000/52 GV 15 HWCP 15% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GS 20 HWCP 20% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 HWS Nylon 66, Finely Crystalline, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | >= 200 °C | >= 392 °F | ISO-R 75 Method B |
Hippe PA 66 Nylon 66 The polyamide with high degree of hardness, stiffness, scuff strength and stability of shape under heat. Preferred polyamide for components subjected to high load and heat stress in electrical, mec.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/2 |
Eurotec® Tecomid® NB40 MR30 NL PA 6 30% mineral reinforced Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHSA NC010 is a heat stabilized lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
Beijing Ranger Chem PBT-201-G15 291 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
Ascend Performance Materials Vydyne® 50BW Nylon 66, Dry as Molded Vydyne® 50BW is a general purpose Nylon 66 resin. Available in natural. Designed for extrusion applications that do not require use of a high-viscosity resin. This resin offers a well-balanced comb.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 179 |
CP-Polymer-Technik Wellamid® 6600 GS 15 HWCP 15% Glass Sphere Filled Nylon 66, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | DAM; ISO 75-1/-2 |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-1/2 |
Eurotec® Tecomid® NB40 KK30 NL IL PA 6 30% glass fiber/mineral reinforced, impact modified, low warpage Excellent stiffness/toughness balanceHigh mechanical strengthVery good thermal stabilityExcellent flammability characteristicsGood electrical propertiesHigh wear resistance and low frictionVery good.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Unannealed; ISO 75-2/B |
Ascend Performance Materials Vydyne® 66Z Nylon 66, DAM Vydyne® 66Z is a high-viscosity PA66 resin suitable for injection-molding and extrusion applications. It is available in natural color only. Vydyne 66Z resin offers high strength, rigidity and toug.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ASTM D648 |
Ashley Polymers Ashlene® 524 Nylon 66 A general purpose toughened Nylon 66.Data provided by the manufacturer |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | ISO 75-2 |
BASF Ultradur® B 4300 K6 30% Glass Bead Filled PBT Description: Is a PBT + ASA, Injection-molding grades containing 30% of glass beads for industrial parts with low warpage.Applications: Precision parts for optical instruments, fuel tank sensor unit.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 200 °C | 392 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Valox® VX5530 PBT (Europe-Africa-Middle East) VALOX VX5530 is a flame retarded, 15% glass fibre reinforced, 10% mineral filled PBT+PC blend with excellent low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |