Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648-95 |
Multibase Multi-Flex® TPO D 4502 C Black Multi-Flex® D 4502 Black is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion.Data provided by Multibase. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 74.8 °C | 167 °F | conditioned @ 50 deg.C; ASTM D648 |
PolyOne Geon™ Vinyl Dry Blend E7755 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 - 120 °C | 167 - 248 °F | Average value: 96.5 °C Grade Count:6 |
Overview of materials for PEN-PET This property data is a summary of similar materials in the MatWeb database for the category "PEN-PET". Each property range of values reported is minimum and maximum values of appropriate MatWeb ent.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-1/-2 |
DSM Arnite® D00 301 PET (European Grade)
(discontinued **) Arnite resins are engineered to provide specific performance in applications where DSM technology can offer value.Arnite Molding resins: Standard Unfilled and Reinforced materialsHigh modulus Flame .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | |
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Petrothene® LR732001 High Density Polyethylene (Blow Molding Grade) ApplicationsThe PETROTHENE LR 7320 series of polyethylene resins exhibits an excellent balance of stiffness and environmental stress crack resistance. Typical applications include bottles for bleac.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
I. Stern 320NB Prime Impact Copolymer Polypropylene, No Break Features:Outstanding impact strength balanced with stiffnessExcellent long term heat aging propertiesWet/dry environment resistanceGood surface glossApplicationsAutomotiveApplianceLawn and GardenRig.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C @Thickness 3.17 mm |
167 °F @Thickness 0.125 in |
un-annealed; ISO 75 |
MRC Polymers MAXTELâ„¢ 600T30IM TPO, 30% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityImpact ModifiedCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Pol.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Flint Hills P5M4R-034 Polypropylene Random Copolymer Features: Radiation resistant. Product does not contain animal derived components. Phthalate-free.Applications: Injection Molding: medical devicesInformation Provided by Flint Hills Resources |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
LyondellBasell Hifaxâ„¢ ETA-3131E Thermoplastic Olefin Resin Key Features: fractional melt flow, medium modulus, extrusion grade thermoplastic olefin resin, excellent impact and stiffness balance, good practical impact, good processabilityApplications: molded.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Noryl V080 PPE+HIPS (Europe-Africa-Middle East) NORYL V080 is an unfilled, flame retardant, high flow material and is halogen free according to VDE/DIN 472 part 815.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
SCG Chemicals EL-Leneâ„¢ H6105JU High Density Polyethylene Injection Molding Key Characteristics:Good processabilityWide service temperatureHigh rigidityGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drinks, bottles, pallet, garbage bins, .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Lubrizol Stat-Rite® X-5076 Static Control High Impact Polystyrene Stat-Rite® X-5076 is a static dissipative, High Impact Polystyrene alloy. Stat-Rite® X-5076 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, p.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-2 |
Borealis RE420MO Polypropylene Random Copolymer, Transparent RE420MO is a specially modified highly-transparent polypropylene random copolymer with medium melt flow rate. This grade is intended for injection molding and stretch blow molding. and is designed .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-1,-2 |
Topas Advanced Polymers TOPAS® 8007S-04 Cyclic Olefin Copolymer (COC) TOPAS® 8007S-04 is a general purpose injection molding grade. It is a glass-clear amorphous polymer with outstanding moisture barrier, chemical resistance, high purity and a non-reactive surface ma.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-1,-2 |
Topas Advanced Polymers TOPAS® 8007X10 Cyclic Olefin Copolymer (COC) TOPAS® 8007X10 is a highly UV-transparent version of our 8007 series of injection molding resins. Like the rest of the 8007 grades, 8007X10 is a glass-clear amorphous polymer with outstanding moist.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D-648-92 |
Lubrizol Stat-Rite® X5166 Static Dissipative Polystyrene Compound Stat-Rite® X5166 is a static dissipative, High-Impact Polystyrene alloy. Stat-Rite® X5166 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, perm.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
A. Schulman POLYPUR™ FPU 1152C Thermoplastic Polyurethane Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | Unannealed (0.250 in); ASTM D648 |
Entec Hypel® PEHD18/.956 HDPE Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-2/B |
ExxonMobil PP8013L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with very high impact strength at low temperature. It is suitable for molding applications like containers and tubs, other rigid packaging, t.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
ExxonMobil PP9074MED Polypropylene Homopolymer Product Description: A highly clarified random copolymer resin designed for injection molding of medical devices suitable for sterilization by high energy radiation.Availability: Europe and North A.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D-648 |
Axiall MP-6510 Rigid PVC, Molding Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM-D648 |
Braskem GV0350 HDPE Blow Molding Polyethylene Copolymer HDPE GV0350 is a high-density polyethylene copolymer that has great molar mass, excellent chemical resistance, and high impact resistance and stiffness. It was developed for the blow-molding of larg.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Braskem Green PE SGF4950 Blow Molding and Monofilament High Density Polyethylene Description: SGF4950 is a high-density polyethylene copolymer, developed for the blow-molding segment. It shows well balanced properties between impact and stiffness, combined with high environmenta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | |
Addcomp PRIEX® 25095 Maleic Anhydride Grafted PP random copolymer Uses: Enhance sealability in bi-oriented polypropylene film packagingIncrease adhesion between metallic or textile wire and polymer coatingAchieve high compatibility between glass or other natural f.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ASTM D648 |
Tipco Tipcolene® FPT 20 PPC - 20% Talc Reinforced Polypropylene Copolymer Compound 20% Talc Reinforced PP CopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 75.0 °C | 167 °F | ISO 75-1/-2 |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT)
(Unverified Data**) Sorona® MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably sourced ingredients by weight. It was initially coded SE38001.Information provided by DuPont.. |