Georgia Gulf MP-6510 is a maximum properties electrical grade PVC injection molding compound processing excellent strength and toughness. In addition, it has good processing stability and surface appearance. It carries a UL 94 V-0/5VA flammability rating, as well as a UL RTI rating.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.32 - 1.38 g/cc
1.32 - 1.38 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 100
100
ASTM D-785
Tensile Strength, Yield 41.4 MPa
6000 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 75.8 MPa
11000 psi
ASTM D-790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D-790
Izod Impact, Notched 1.60 J/cm

@Thickness 3.17 mm,
Temperature -20.0 °C
3.00 ft-lb/in

@Thickness 0.125 in,
Temperature -4.00 °F
ASTM D-256
9.61 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
18.0 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256
Gardner Impact 22.6 J

@Temperature 23.0 °C
16.7 ft-lb

@Temperature 73.4 °F
1/2" R Tup, 67 mil
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 75.0 °C
167 °F
ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 70.0 °C
158 °F
ASTM D-648
UL RTI, Electrical 90.0 °C

@Thickness 1.40 mm
194 °F

@Thickness 0.0551 in
UL-746B
UL RTI, Mechanical with Impact 85.0 °C

@Thickness 1.40 mm
185 °F

@Thickness 0.0551 in
UL-746B
UL RTI, Mechanical without Impact 90.0 °C

@Thickness 1.40 mm
194 °F

@Thickness 0.0551 in
UL-746B
Flammability, UL94 5VA
5VA
Oxygen Index 36 %
36 %
ASTM D-2863
Descriptive Properties Value Comments
Flow Ratio (Distance/Wall Thickness, 390-400°F) 180
Georgia Gulf Test
UL Weatherability Rating F(1)
UL-746C
Users viewing this material also viewed the following: