Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
Mytex Polymers AS14KW-02 Polypropylene, Talc filled, Compounded Description: Talc filled compounded polypropylene produced for automotive interior applications using Mytex® Technology.Key Applications: General purpose interiorInformation provided by Mytex Polym.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
LyondellBasell SEQUEL® E5000 TPO Description: SEQUEL® E5000 thermoplastic olefinic elastomer (TPO) is designed for extrusion applications that require high mechanical stiffness, thermal stability, good low-temperature properties.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648-97 |
Ipiranga Petrochem PH 0242 Polypropylene The production of polypropylene (PP) employs Spheripol technology from Montell / Italy. This technology has been acclaimed all over the world and is known as clean technology, because it does not pr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ISO 75-1,-2 |
Ineos ABS Lustran® Ultra 4115 ABS Pellets (a-methylstyrene-SAN / PC-modified), Very High Heat Grade Lustran® Ultra 4115 is very high heat grade with high impact resistance and is PC-modified. It is used for the production of molded plastic articles. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ISO Method 180 |
LyondellBasell Astryn BB73F Polypropylene Copolymer, Mineral Filled Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled, high rigidity, good impact strength, good dimensional stability, good scratch and mar resistance, excellent processability,.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East) LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP NL001 PC+ABS (Europe-Africa-Middle East) LNP LUBRICOMP* NL001 is a wear resistant PC+ABS blend, suitable for thin wall applications. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C @Thickness 3.20 mm |
237 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC PPCOMPOUND 55T1030 PP SABIC® PPcompound 55T1030 is a general purpose, talc filled, heat stabilized copolymer polypropylene compound. This compound exhibits very high impact, and is suitable for multiple processing met.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C @Thickness 3.20 mm |
237 °F @Thickness 0.126 in |
ASTM D648 |
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Asia Pacific) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics Xenoy® X3515 PC+POLYESTER (Europe-Africa-Middle East) Flame Retardant, Impact Modified, Opaque, Designed for outdoor telecommunication enclosure applications.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ISO 75 |
Styrolution Novodur® 4115 ABS Novodur Ultra 4115 is a PC modified high heat injection molding grade. It provides good heat resistance combined with high impact strength.Information provided by Styrolution |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP STAT-KON 9X02785 PC LNP STAT-KON* 9X02785 is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | 0.250 inch; Unannealed; ASTM D648 |
TPI Porene® KU900 Super High Heat ABS INJECTION MOLDING. ELECTRICAL PARTS, AUTOMOTIVE APPLICATIONS, HOUSEHOLD GOODS, TOYSPorene® is a registered trademark of Thai Petrochemical Industry Co. LTD. Information provided by Dayson Polymer.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | 120°C per hour; ISO 752 |
Total PPC 10642 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 10642 is a nucleated antistatic heterophasic copolymer with high Melt Flow index of 44 g/10 min.Polypropylene PPC 10642 is characterized by high fluidity with good mechanical prope.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | Unannealed; ASTM D648 |
ExxonMobil AP3N Polypropylene Impact Copolymer Product Description: A medium impact copolymer resin designed for appliance applications requiring good stiffness and fast cycle time.Availability: Asia Pacific Features:Fast Molding CycleHigh Glos.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
Aclo Accutech Polypropylene Homopolymer HP0339W20L Wollastonite Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM-D648 |
Braskem PH 0242 HOMO Polypropylene Homopolymer PH 0242 is a low melt flow rate homopolymer produced by compression molding. This resin exhibits excellent processability and excellent stiffness/impact strength balance. Its applications include co.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | |
Arkema Group Appryl® CWE 1020 Polypropylene, 20% Talc Filled Compound of a PP copolymer and 20% aesthetic talc. This grade has been specially developed for interior trim automotive applications, that required an excellent scratch resistance associated with a .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
Braskem CP 405XP Compression Molding Polypropylene Heterophasic Copolymer Bottle caps for carbonated beverages.Information provided by Braskem. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
Aclo Accutech Polypropylene Copolymer CP0436T40L Talc Reinforced |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | 90 Minute UV Cure + Thermal; ASTM D648 |
3D Systems Accura® SI 40 Plastic for the SLA® 500 System Accura 40 "Ar" or "Hc" type materials - for the SLA 500 system. Mimics Nylon 6:6ApplicationsHigh temperature testing:Under hood bolt-on testingWind tunnel testingHVAC testingPrototyping and testing .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFLAM™ E-15086-1B Mineral Impact Modified, Low Warp Polypropylene Black DescriptionPolyfort® E-15086-1B is a mineral impact modified low warp polypropylene black.Information provided by A. Schulman. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 114 °C | 237 °F | ASTM D648 |
A. Schulman POLYFORT™ PP 3052UX Impact Resistant Copolymer DescriptionPolyfort® PP 3052UX is a UV stabilized extra high flow impact resistant copolymer with a relatively high stiffness.Information provided by A. Schulman. |