Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 100 °C |
4.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
H.C. Starck MoCu 65/35 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
H.C. Starck MoCu 70/30 Molybdenum-Copper Composite Material Description of Product: Molybdenum-copper composite materials are produced by copper infiltration of porous sintered molybdenum. They are available with different copper contents (15 - 35 %). A t.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott GG420 Long Pass Filter Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG385, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG6.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-BAK1 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 300 °C |
4.78 µin/in-°F @Temperature 68.0 - 572 °F |
|
Schott N-LASF45 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.78 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott N-SF8 Glass Information Provided by SCHOTT North America, Inc. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature -30.0 - 70.0 °C |
4.78 µin/in-°F @Temperature -22.0 - 158 °F |
|
Schott BG12 Band Pass Filter Ionically colored glass. Data provided by the manufacturer, Schott Glas Mainz. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 100 °C |
4.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET 75A CP Titanium (ASTM Grade 4) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4901. Germany Engineering: 3.7065. Germany Aerospace: 3.7064. France: T-60. UK Aerospace Specification BS TA. 6.Features.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 100 °C |
4.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET CP Titanium (ASTM Grade 3) Commercially Pure Titanium. Industry Specifications: USA Aerospace: AMS 4900. Germany Aerospace: 3.7055. France: T-50. UK Aerospace Specification DTD 5023, 5273.Features: The mechanical properti.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 °C |
4.78 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al), Anneal Strip/Sheet High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 °C |
4.78 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 482°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 °C |
4.78 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 15-3 Titanium Alloy (Ti-15V-3Cr-3Sn-3Al); Aged at 538°C High-Strength, Cold Formable Strip AlloyIndustry Specifications: USA Aerospace: AMS 4914A.Features: Cold formable and weldable, this strip alloy is primarily used for aircraft ducting, pressure vess.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 100 °C |
4.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1) Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 - 100 °C |
4.78 µin/in-°F @Temperature 68.0 - 212 °F |
|
TIMET TIMETAL® 50A CP Titanium (ASTM Grade 2) Commercially Pure Titanium.Industry Specifications: USA Aerospace: AMS 4902, 4941. Germany Engineering: 3.7035. Germany Aerospace: 3.7034. France: T-40. UK Aerospace Specifications BS TA. 2, 3,.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 °C |
4.78 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 °C |
4.78 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Beta Forged Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wi.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 30.0 - 400 °C |
4.78 µin/in-°F @Temperature 86.0 - 752 °F |
|
Ametek Tungsten-Copper Composites AWC 8020 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
CTE, linear | 8.60 µm/m-°C @Temperature 20.0 °C |
4.78 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, .. |