Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1)

Category Metal , Nonferrous Metal , Titanium Alloy , Unalloyed/Modified Titanium
Manufacturer TIMET
Trade Name TIMETAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF TIMET TIMETAL® 35A CP Titanium (ASTM Grade 1).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Commercially Pure Titanium.Industry Specifications: Germany Engineering: 3.7025. Germany Aerospace: 3.7024. France: T-35. UK Aerospace Specification: BS TA. 1.Features: The mechanical properties of CP titanium are influenced by small additions of oxygen and iron. By careful control of these additions, the various grades of commercially pure titanium are produced to give properties suited to different applications. TIMETAL 35A contains the lowest oxygen and iron levels, producing the most formable grade of material. It has the highest purity, lowest strength, and best room-temperature ductility and formability of the four ASTM commercially pure grades. 35A should be used where maximum formability is required such as in explosive bonding and plate type heat exchangers. It exhibits excellent corrosion resistance in highly oxidizing to mildly reducing environments, including chlorides. It has good impact properties at low temperatures. In addition, TIMETAL 35A can be easily welded, machined, cold worked, hot worked, and cast. It is nonmagnetic.Typical heat treatment for this alloy: Anneal at 700°C for 1 hour and air cool. Stress Relieve at 500°C for 30 mins and air cool.Data provided by TIMET.
Physical Properties Metric English Comments
Density 4.51 g/cc
0.163 lb/in³
Typical
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 345 MPa
50000 psi
Typical
Tensile Strength, Yield 220 MPa

@Strain 0.200 %
31900 psi

@Strain 0.200 %
Typical
Elongation at Break 35 %
35 %
Typical
Reduction of Area 70 %
70 %
Typical
Modulus of Elasticity 105 - 120 GPa
15200 - 17400 ksi
Typical
Fatigue Strength 123 MPa

@# of Cycles 1.00e+7
17800 psi

@# of Cycles 1.00e+7
Notched, Kt=3; rotating bend
193 MPa

@# of Cycles 1.00e+7
28000 psi

@# of Cycles 1.00e+7
Smooth, Kt=1; rotating bend
Bend Radius, Minimum 2.0 t

@Thickness 2.00 mm
2.0 t

@Thickness 0.0787 in
Typical; sheet
Thermal Properties Metric English Comments
CTE, linear 8.60 µm/m-°C

@Temperature 20.0 - 100 °C
4.78 µin/in-°F

@Temperature 68.0 - 212 °F
9.50 µm/m-°C

@Temperature 20.0 - 300 °C
5.28 µin/in-°F

@Temperature 68.0 - 572 °F
9.70 µm/m-°C

@Temperature 20.0 - 500 °C
5.39 µin/in-°F

@Temperature 68.0 - 932 °F
Thermal Conductivity 21.97 W/m-K
152.5 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 425 °C
797 °F
Continuous
540 °C
1000 °F
Intermittent
Beta Transus 890 °C
1630 °F
Component Elements Properties Metric English Comments
Carbon, C <= 0.080 %
<= 0.080 %
Hydrogen, H <= 0.015 %
<= 0.015 %
Iron, Fe <= 0.20 %
<= 0.20 %
Nitrogen, N <= 0.030 %
<= 0.030 %
Oxygen, O <= 0.18 %
<= 0.18 %
Titanium, Ti >= 99.1 %
>= 99.1 %
Calculated as remainder
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000450 ohm-cm
0.0000450 ohm-cm
Users viewing this material also viewed the following: