| Category | Ceramic , Glass |
| Manufacturer | Schott North America |
| Trade Name | |
| Port | Ningbo port,China |
| Trade Terms | EXW, FOB, CFR, CIF |
| Payment Terms | L/C, T/T, PayPal |
| Download PDF | Schott N-BAK1 Glass.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 3.19 g/cc | 0.115 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Knoop Microhardness | 530 | 530 | .1/20 |
| Modulus of Elasticity | 73.0 GPa | 10600 ksi | |
| Poissons Ratio | 0.252 | 0.252 | |
| Shear Modulus | 29.0 GPa | 4210 ksi | calculated |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 7.60 µm/m-°C <br>@Temperature -30.0 - 70.0 °C |
4.22 µin/in-°F <br>@Temperature -22.0 - 158 °F |
|
| 8.60 µm/m-°C <br>@Temperature 20.0 - 300 °C |
4.78 µin/in-°F <br>@Temperature 68.0 - 572 °F |
||
| Specific Heat Capacity | 0.687 J/g-°C | 0.164 BTU/lb-°F | |
| Thermal Conductivity | 0.795 W/m-K | 5.52 BTU-in/hr-ft²-°F | |
| Transformation Temperature, Tg | 592 °C | 1100 °F |
| Optical Properties | Metric | English | Comments |
|---|---|---|---|
| Refractive Index | 1.5725 <br>@Wavelength 587.6 nm |
1.5725 <br>@Wavelength 587.6 nm |
n<sub>d</sub> |
| 1.57487 <br>@Wavelength 546.1 nm |
1.57487 <br>@Wavelength 546.1 nm |
n<sub>e</sub> | |
| Transmission, Visible | 99.3 % <br>@Thickness 10.0 mm,<br> Wavelength 380 nm |
99.3 % <br>@Thickness 0.394 in,<br> Wavelength 380 nm |
|
| 99.6 % <br>@Thickness 10.0 mm,<br> Wavelength 405 nm |
99.6 % <br>@Thickness 0.394 in,<br> Wavelength 405 nm |
||
| 99.6 % <br>@Thickness 10.0 mm,<br> Wavelength 460 nm |
99.6 % <br>@Thickness 0.394 in,<br> Wavelength 460 nm |
||
| 99.8 % <br>@Thickness 10.0 mm,<br> Wavelength 580 nm |
99.8 % <br>@Thickness 0.394 in,<br> Wavelength 580 nm |
||
| 99.9 % <br>@Thickness 10.0 mm,<br> Wavelength 700 nm |
99.9 % <br>@Thickness 0.394 in,<br> Wavelength 700 nm |
||
| IR Transmittance | 80.6 % <br>@Thickness 10.0 mm,<br> Wavelength 2500 nm |
80.6 % <br>@Thickness 0.394 in,<br> Wavelength 2500 nm |
|
| 99.4 % <br>@Thickness 10.0 mm,<br> Wavelength 1530 nm |
99.4 % <br>@Thickness 0.394 in,<br> Wavelength 1530 nm |
||
| UV Transmittance | 1.4 % <br>@Thickness 10.0 mm,<br> Wavelength 280 nm |
1.4 % <br>@Thickness 0.394 in,<br> Wavelength 280 nm |
|
| 34.5 % <br>@Thickness 10.0 mm,<br> Wavelength 300 nm |
34.5 % <br>@Thickness 0.394 in,<br> Wavelength 300 nm |
||
| 92.4 % <br>@Thickness 10.0 mm,<br> Wavelength 334 nm |
92.4 % <br>@Thickness 0.394 in,<br> Wavelength 334 nm |
||
| 99.1 % <br>@Thickness 10.0 mm,<br> Wavelength 370 nm |
99.1 % <br>@Thickness 0.394 in,<br> Wavelength 370 nm |
| Chemical Properties | Metric | English | Comments |
|---|---|---|---|
| Acid Class, SR | 3.3 | 3.3 | |
| Alkali Class, AR | 1.2 | 1.2 | |
| Stain Resistance Class, FR | 1.0 | 1.0 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| B | 1 | |
| Climatic Resistance Test CR | 2 | |
| HG | 2 | |
| K (10-6mm2/N) | 2.62 | |
| Phosphate Resistance PR | 2 | |
| T1013.0 (°C) | 592 | |
| T107.6 (°C) | 746 |