Schott GG420 Long Pass Filter

Category Ceramic , Glass , Filter , Optical
Manufacturer Schott Glas Mainz
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Schott GG420 Long Pass Filter.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Colloidally colored glass. Data provided by the manufacturer, Schott Glas Mainz.Similar glasses include GG395, GG400, GG385, GG435, GG455, GG475, GG495, OG515, OG530, OG550, OG570, OG590, RG610, RG630, RG645, RG665, RG695, RG715, RG780, RG830, RG850, RG1000, WG225, WG280, WG295, WG305, WG320
Physical Properties Metric English Comments
Density 2.76 g/cc
0.0997 lb/in³
Thermal Properties Metric English Comments
CTE, linear 7.70 µm/m-°C

@Temperature -30.0 - 70.0 °C
4.28 µin/in-°F

@Temperature -22.0 - 158 °F
8.60 µm/m-°C

@Temperature 20.0 - 300 °C
4.78 µin/in-°F

@Temperature 68.0 - 572 °F
Transformation Temperature, Tg 586 °C
1090 °F
Glass Temperature Coefficient 0.080
0.080
Optical Properties Metric English Comments
Refractive Index 1.53

@Wavelength 1014 nm
1.53

@Wavelength 1014 nm
Hg
1.54

@Wavelength 587.6 nm
1.54

@Wavelength 587.6 nm
He
1.56

@Wavelength 435.8 nm
1.56

@Wavelength 435.8 nm
Hg
Transmission, Visible <= 0.70 %

@Wavelength 400 - 410 nm
<= 0.70 %

@Wavelength 400 - 410 nm
90 %

@Wavelength 500 - 510 nm
90 %

@Wavelength 500 - 510 nm
Internal transmittance of 99% from 500-510 nm
IR Transmittance 91 %

@Wavelength 710 - 1600 nm
91 %

@Wavelength 710 - 1600 nm
Internal transmittance of 100%  from 710-1600 nm.
UV Transmittance 0.0010 %

@Wavelength 200 - 400 nm
0.0010 %

@Wavelength 200 - 400 nm
Internal transmittance of 0.001% from 200-400 nm.
Reflection Coefficient, Visible (0-1) 0.90
0.90
Chemical Properties Metric English Comments
Acid Class, SR 1
1
Alkali Class, AR 2.3
2.3
Stain Resistance Class, FR 0.0
0.0