Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 18.0 µm/m-°C @Temperature 0.000 - 150 °C |
10.0 µin/in-°F @Temperature 32.0 - 302 °F |
X-Direction; IPC-TM-650 2.1.41 |
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material SYRON™ 7000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7000 is thermally stable, with a .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 400 °C |
10.0 µin/in-°F @Temperature 752 °F |
|
Outokumpu 4307 Cr-Ni Austenitic Stainless Steel General purpose steel with good corrosion resistance.Applications: Wide variety of applications in construction, chemical, petroleum, automobile, and domestic appliance markets.Available in hot roll.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 500 °C |
10.0 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4318 Cr-Ni Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled strip/sheet (CPP) and cold rolled strip sheet forms. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 500 °C |
10.0 µin/in-°F @Temperature 932 °F |
|
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 200 - 300 °C |
10.0 µin/in-°F @Temperature 392 - 572 °F |
ASTM E831 |
3M Dyneon™ CC622 PTFE 10% Graphite Filled
(discontinued **) Product Form: Black, pelletized free-flowing powder. Applications include bearings, ring seals.Data provided by Dyneon. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.0 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel CLC 17.12.2 L 2% Mo Containing 18 Cr –10 Ni Austenitic Stainless Steel Description: CLC 17-12-2L is one of the basic grade of the stainless steels range. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 300 °C |
10.0 µin/in-°F @Temperature 68.0 - 572 °F |
|
Industeel CLC 17.12.2 Ti Titanium Stabilized 18Cr-11Ni-2Mo Austenitic Stainless Steel CLC 17-12-2Ti is a Titanium stabilized austenitic stainless steel. 2% Molybdenum bearing ensures better corrosion resistance than CLC 18-9 L grade, particularly regarding to uniform and localized co.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 500 °C |
10.0 µin/in-°F @Temperature 68.0 - 932 °F |
|
Industeel CLC 18.12.4 LN 3%Mo Austenitic Stainless Steel with Nitrogen Addition Description: CLC 18-12-4LN (317LN) is a Nitrogen alloyed austenitic stainless steel with a 3% Mo minimum addition (>4%). Alloys CLC 18-12-4LN (317LN) exhibit austenitic microstructure free of delete.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 600 °C |
10.0 µin/in-°F @Temperature 68.0 - 1110 °F |
|
Industeel SIRIUS 310 25% Cr - 0.6% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 310 grade is a fully austenitic stainless steel containing 25% Cr, 0.6% Si and 20% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resi.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 400 °C |
10.0 µin/in-°F @Temperature 68.0 - 752 °F |
|
Industeel SIRIUS 314 25% Cr - 1.8% Si Heat Resistant Stainless Steel Description: CLI SIRIUS 314 grade is a fully austenitic stainless steel containing 25% Cr, 20% Ni and 1.8% Si. The alloy is designed for high temperature corrosion resistance applications even in se.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 10% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 358 °C |
10.0 µin/in-°F @Temperature 68.0 - 676 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 60% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 358 °C |
10.0 µin/in-°F @Temperature 68.0 - 676 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, Annealed (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 100 - 200 °C |
10.0 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature -50.0 - 50.0 °C |
10.0 µin/in-°F @Temperature -58.0 - 122 °F |
Axial; ASTM E831 |
Chevron Phillips Xtel® XK2040 Polyphenylene Sulfide Alloy
(discontinued **) Natural Color Polyphenylene Sulfide AlloyXtel™ XK2040 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties alo.. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 100 - 200 °C |
10.0 µin/in-°F @Temperature 212 - 392 °F |
Axial; ASTM E831 |
Chevron Phillips Xtel® XK2140 Polyphenylene Sulfide Alloy
(discontinued **) Black Polyphenylene Sulfide AlloyXtel™ XK2140 is a high performance, glass fiber reinforced, PPS-based alloy developed to provide excellent mechanical strength and electrical properties along with .. |
|||
CTE, linear | 18.0 µm/m-°C @Temperature 20.0 - 316 °C |
10.0 µin/in-°F @Temperature 68.0 - 601 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201L, 40% Cold Work (UNS S20103) Allegheny Ludlum Types 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201L provides advantages over the 18-8 grades in certain applications. Lower cost manganese .. |