Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -40.0 - 40.0 °C |
63.3 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP LUBRICOMP KP004 Acetal LNP LUBRICOMP* KP004 is a compound based on Acetal Copolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -30.0 - 30.0 °C |
63.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON RX08408 PA 66 LNP* STAT-KON* RX08404 is a compound based on Nylon 66 containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -30.0 - 30.0 °C |
63.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Stat-kon RX08408_NA1D004 PA 66 LNP* Stat-Kon* RX08404_NA1D004 is a compound based on Nylon 66 containing Carbon Powder. Characteristics of this grade include: Electrically Conductive, High Impact.This data was supplied by SABI.. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature 23.0 - 60.0 °C |
63.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp HF00ASU PA11 (Europe-Africa-Middle East) LNP* THERMOCOMP* HF00ASU is a compound based on PA11 resin containing Glass Fiber. Added features include; Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature 23.0 - 60.0 °C |
63.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp MB006SU PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MB006SU is a compound based on Polypropylene resin containing Glass Bead. Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europe-Af.. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -30.0 - 30.0 °C |
63.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP QF007 PA 6/10 LNP* THERMOCOMP* QF007 is a compound based on Nylon 6/10 resin containing 35% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature 23.0 - 60.0 °C |
63.3 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starpylen MB006SU PP, Glass Bead Filled, Injection Molding Resin Starpylen MB006SU is a Glass Bead Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
CTE, linear, Transverse to Flow | 114 µm/m-°C @Temperature -30.0 - 30.0 °C |
63.3 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP VERTON PX06418 PA 6 LNP* VERTON* PX06418 is a compound based on Nylon 6 containing proprietary fillers. Added features of this grade are: Heat Stabilized, Structural. |