Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
53.9 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
53.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP MX91206 PP LNP* Lubricomp* MX91206 is a compound based on Polypropylene containing proprietary fillers. Added feature of this grade is: Wear Resistant. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP WG003 PBT (Europe-Africa-Middle East) LNP* LUBRICOMP* WG003 is a compound based on Polybutylene Terephalate resin cantain Graphite. Added features include: Internally Lubricated. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON AE003 ABS (Europe-Africa-Middle East) LNP* STATKON* AE003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features inclurde : Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp PFB139E PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB139E is a compound based on PA 6 resin containing Glass Fiber, Glass Bead, Flame Retardant. Added features include; Flame Retardant, Easy Molding.This data was supplied by SABIC-.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® K3501 PBT Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
53.9 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® K3501 PBT (Europe-Africa-Middle East) Unfilled PBT, Hydrollytically Stable, Heat Stabilized, Impact Modified. A hydrollytically stable grade designed for improved performance under heat/humidity environments. Targeted at automotive unde.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C | 53.9 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 520MP NC010 Acetal (POM)
(Unverified Data**) 20% Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 520MP is a medium viscosity acetal homopolymer containing 20% Teflon PTFE Micropowder. It is designe.. |
|||
CTE, linear, Transverse to Flow | 97.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
53.9 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Starflam PFB139E PA6, Glass Fiber/Bead Filled, Flame Retardant, Injection Molded Starflam PFB139E is a Flame Retardant Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding Resin (also known as PFB1013Z590)Information provided by Eurostar. |