Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Geloy XTPM302 ASA+PC (Europe-Africa-Middle East) XTPM302 is a general purpose ASA/PC injection moulding grade, available in various colors.Typical properties measured on natural material.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP LUBRICOMP RFL33 PA 66 (Europe-Africa-Middle East) LNP* Lubricomp* RFL33 is a compound based on Nylon 66 resin containing Glass Fiber, PTFE. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
52.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP STAT-KON KX96321 POM LNP* STAT-KON* KX96321 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® VX5005 PBT (Europe-Africa-Middle East) VALOX VX5005 is a 5% glass fibre reinforced, impact modified PBT+PC blend with low warpage characteristics.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-2 |
SABIC Innovative Plastics Xenoy® 5220U PBT+PC (Europe-Africa-Middle East) Unreinforced PBT+PC alloy. Improved retention of mechanical properties under UV. Excellent low temperature/chemical |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP QC006 PA6.10 (Europe-Africa-Middle East) LNP * THERMOCOMP* QC006 is a compound based on PA610 resin containing Carbon Fiber. Added features include; Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 100 °C |
52.8 µin/in-°F @Temperature -40.0 - 212 °F |
ASTM E831 |
Styron MAGNUMâ„¢ 375 HH Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection moldingApplications: Automotive interior trim applications requiring low volatile organic compounds (VOC)Information provided by.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 100 °C |
52.8 µin/in-°F @Temperature -40.0 - 212 °F |
ASTM E831 |
Styron MAGNUMâ„¢ 375 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: High Heat, Low Gloss, Medium Impact ABS resin for injection molded automotive interior trim applications.Applications: Chrysler-MSDB-191Ford-WSB-M4D690-AGM-GMP.ABS.009Information provided .. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics NORYL PPX PPX640 PPE+PP (Europe-Africa-Middle East) PPX640 is a 40% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. NSF Standard 61 Compliant (color limited)... |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ISO 11359-2 |
SABIC Innovative Plastics Valox® SHF4930 PBT Super high flow FR PBT grade with 15% Glass reinforced |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP PF004 PA 6 (Europe-Africa-Middle East) 20% glass fibre reinforced Polyamide 6 injection moulding resin. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 44 Polycarbonate/ABS Blend Easier flowing than BAYBLEND T 45 MN.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 20.0 °C |
52.8 µin/in-°F @Temperature 68.0 °F |
|
Covestro Bayblend® T 45 MN Polycarbonate/ABS Blend High impact and notched impact strength, little risk of brittle fracture, high dimensional accuracy, good platable.Information provided by Bayer.As of 1 September 2015, Bayer MaterialScience was sep.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C | 52.8 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Rynite® FR515 BK507 Polyethylene Terephthalate (PET)
(Unverified Data**) 15% Glass Reinforced Flame Retardant Polyethylene Terephthalate Rynite FR515 BK507 is a flame retardant 15% glass reinforced modified polyethtylene terephthalate. Recognized by UL as UL94V-0 at 0.8m.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C | 52.8 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G30L NC010 Nylon 66
(Unverified Data**) 30% Glass Reinforced Polyamide 66Zytel 70G30L NC010 is a 30% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 °C |
52.8 µin/in-°F @Temperature -40.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 °C |
52.8 µin/in-°F @Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 95.0 °C |
52.8 µin/in-°F @Temperature 203 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 80G33L NC010 Nylon 66
(Unverified Data**) 33% Glass Reinforced Toughened Polyamide 66 Zytel 80G33L NC010 is a 33% glass fiber reinforced polyamide 66 resin with outstanding impact resistance developed using DuPont Super Tough technology.Inf.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C | 52.8 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® FG70G30HSR3 BK309 Nylon 66
(Unverified Data**) Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 55.0 - 160 °C |
52.8 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 55.0 - 160 °C |
52.8 µin/in-°F @Temperature 131 - 320 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN FR52G30NHF BK337 Polyphthalamide (PPA) 30% Glass Reinforced Flame Retardant Non-Halogenated PPA High Performance Polyamide with Improved Flow Zytel HTNFR52G30NHF BK337 is a 30% glass reinforced flame retardant lubricated high performance.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide AG4 PA66, 20% Glass Filled, Injection Molded AG4 is a 20% Glass Fiber Reinforced Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C | 52.8 µin/in-°F | ISO 11359-1/-2 |
EMS-Grivory Grivory® TR 90 TL PAMACM12 Product description: Grilamid TR 90 TL is a transparent thermoplastic polyamide based on aliphatic, cycloaliphatic and aromatic blocks. The special characteristic of Grilamid TR 90 TL is the high st.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® A3 GF 30 (2397) PA 6.6 Dry, 30% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature 23.0 - 80.0 °C |
52.8 µin/in-°F @Temperature 73.4 - 176 °F |
ISO 11359-1/2 |
Akro-Plastic Akromid® B3 GF 30 (2472) PA 6 Dry, 30% Glass Filled AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur.. |
|||
CTE, linear, Transverse to Flow | 95.0 µm/m-°C @Temperature -40.0 - 40.0 °C |
52.8 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics LNP Stat-kon MX01767C PP LNP* Stat-Kon* MX01767C is a compound based on Polypropylene containing Proprietary Fillers. Charactiers of this grade are Statically Conductive, Clean Compound System.This data was supplied by SAB.. |