Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar DN101 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 61.0 µm/m-°C | 33.9 µin/in-°F | |
Idemitsu Kosan Xarec® WA 204 SPS, 20% Glass Filled Crystalline Polymer, Glass Filled, Impact Modified. Used in Automotive and Industrial applications. |
|||
CTE, linear, Transverse to Flow | 61.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRICOMP RCL34 PA 66 LNP* LUBRICOMP* RCL34 is a compound based on Nylon 66 containing 20% Carbon Fiber, 15% PTFE. Added features of this grade includes: Wear Resistant, Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 61.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP RX10408H PA 66 LNP* Thermocomp* RX10408H is a compound based on Nylon 66 containing Proprietary Fillers. Characteristics are: Radiopacity and Healthcare. |
|||
CTE, linear, Transverse to Flow | 61.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP 2F005 ETFE LNP* Thermocomp* 2F005 is a fluoropolymer compound based on ETFE containing 25% Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 61.0 µm/m-°C @Temperature 20.0 °C |
33.9 µin/in-°F @Temperature 68.0 °F |
|
Toyobo TS501 PPS, 50% Glass Fiber Reinforced Key Feature: High stiffnessHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology developed by Toyobo. Excellent physical, e.. |
|||
CTE, linear, Transverse to Flow | 61.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
33.9 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Americas region. |