Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 89.0 µm/m-°C
49.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 2131/20 H2.0 900051 Nylon 6, 20% Glass Fiber
PA 6, injection molding grade, 20% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, good heat-ageing resistance and weather resistance
CTE, linear, Transverse to Flow 89.0 µm/m-°C
49.4 µin/in-°F
ISO 11359-1/-2
Lanxess Durethan® DP 2131/20 W1 901317 Nylon 6, 20% Glass Fiber
PA 6, injection molding grade, 20% glass fibers, better surface finish and resistance to alcoholic calcium chloride-solution than BKV 20 H2.0, weather resistance, good heat-ageing resistance
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
49.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP LUBRICOMP RFG16 PA 66 (Europe-Africa-Middle East)
LNP* LUBRICOMP* RFG16 is a compound based on PA 66 resin containing Glass Fiber, Graphite. Added features include: Internally Lubricated.
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
49.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Lubricomp WBG16 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WBG16 is a compound based on Polybutylene Terephalate resin containing Glass Bead, Graphite.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
49.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP WFL34 PBT
LNP LUBRICOMP* WFL34 is a compound based on PBT resin containing 20% Glass Fiber, 15% PTFE. Added feature of this grade is: Wear Resistant.
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
49.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 4X08423 FP-P (PFA)
LNP* THERMOCOMP* 4X08423 is a compound based on PFA resin containing Glass Fiber.
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
49.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP AB002 ABS
LNP* THERMOCOMP* AB002 is a compound based on ABS resin containing 10% Glass Bead.
CTE, linear, Transverse to Flow 89.0 µm/m-°C
49.4 µin/in-°F
ISO 11359-1/-2
DuPont Performance Polymers Sorona® 3015GV NC010 Polytrimethylene Terephthalate (PTT)
15% Glass Reinforced Renewably Sourced Polytrimethylene Terephthalate Sorona 3015GV NC010 is a 15% glass reinforced PTT resin containing 31% renewably sourced ingredients by weight (37% based on pol..
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
49.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
Eurostar Staramide BG6ST43 PA6, 30% Glass Fiber Filled, Impact Modified, Injection Molded
BG6ST43 is an Impact Modified and Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier.
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature 20.0 °C
49.4 µin/in-°F

@Temperature 68.0 °F
Arkema Group Orgalloy® RS 66K15LT Nylon 66 Alloy, Mineral/Impact Grade (Conditioned)
RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie..
CTE, linear, Transverse to Flow 89.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
49.4 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP Stat-kon PX98038 PA 6 (Europe-Africa-Middle East)
LNP* STATKON* PX98038 is a compound based on PA6 resin containing Carbon Fiber, Glass Fiber, Flame Retardant. Added features include : Flame Retardant, Electrically Conductive, Heat Stabilized.This ..
Copyright © lookpolymers.com All Rights Reserved