Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 20.0 °C |
32.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastapak 9921W PET
(discontinued **) Unreinforced. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 20.0 °C |
32.8 µin/in-°F @Temperature 68.0 °F |
|
Eastman Eastar GN101 PETG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 0.000 - 100 °C |
32.8 µin/in-°F @Temperature 32.0 - 212 °F |
ASTM E381 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
CTE, linear, Transverse to Flow | 59.0 - 78.1 µm/m-°C | 32.8 - 43.4 µin/in-°F | Average value: 67.6 µm/m-°C Grade Count:15 |
Overview of materials for Polycarbonate, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Impact Modified". Each property range of values reported is minimum and maximum values of.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Thermocomp CF004 PS (Europe-Africa-Middle East) LNP* Thermocomp* CF004 is a compound based on Polystyrene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP GF006 PSU (Europe-Africa-Middle East) LNP* THERMOCOMP* GF006 is a compound based on Polysulfone resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP RF00C PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RF00C is a compound based on Nylon 66 resin containing Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 60.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP UF007AS PPA (Europe-Africa-Middle East) LNP* THERMOCOMP* UF007AS is a compound based on Polyphthalamide resin containing Glass Fiber. Added features include Heat Stabilized . |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
32.8 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP THERMOCOMP WFB62 PBT LNP* THERMOCOMP* WFB62 is a compound based on PBT resin containing 10% Glass Fiber, 10% Glass Bead. Added feature of this grade is: Low Warpage. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® ET3032 FR Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature -40.0 - 23.0 °C |
32.8 µin/in-°F @Temperature -40.0 - 73.4 °F |
DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50LWSF BK702A Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Low Warpage and High Stiffness Information provided by DuPont Performance Polymers |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C @Temperature 23.0 - 55.0 °C |
32.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Covestro Bayblend® FR410 MT Rubber Modified PC Blend, 10% Mineral Filled Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | z, before Tg; IPC TM-650 2.4.24 |
Arlon 25FR Low-Cost Ceramic Hydrocarbon High Frequency, Low Loss Thermoset Laminate and Prepreg for Double-sided, Multilayer and Mixed Dielectric Printed Circuit BoardsLow loss ceramic-filled thermoset resinTight dielectric tolerance cont.. |
|||
CTE, linear, Transverse to Flow | 59.0 µm/m-°C | 32.8 µin/in-°F | TMA |
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound Medium flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited f.. |