Thermal Properties Metric English Comments
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP DFL36EU PC
LNP* Lubricomp* DFL36EU is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features include: Internally Lubricated, Easy Molding and UV Stabilized.
CTE, linear, Transverse to Flow 43.0 - 67.0 µm/m-°C

@Temperature 50.0 - 300 °C
23.9 - 37.2 µin/in-°F

@Temperature 122 - 572 °F
Average value: 54.5 µm/m-°C Grade Count:2
Overview of materials for Thermoplastic Polyimide, Carbon Fiber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va..
CTE, linear, Transverse to Flow 43.0 µm/m-°C
23.9 µin/in-°F
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRICOMP RCL26 PA6.6
LNP* LUBRICOMP* RCL26 is a compound based on Nylon 66 containing 30% Carbon Fiber, 10% PTFE. Added features of this grade include: Wear Resistant, Electrically Conductive.
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP STAT-KON EX11318C PEI (Asia Pacific)
LNP* Stat-Kon* EX11318C is a polyetherimide compound reinforced with carbon fiber for good stiffness, dimension stability and has extremely high level of cleanliness for the most demanding applicati..
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature 23.0 - 60.0 °C
23.9 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP EF006 PEI (Europe-Africa-Middle East)
LNP* THERMOCOMP* EF006 is a compound based on Polyetherimide resin containing Glass Fiber.
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -40.0 - 40.0 °C
23.9 µin/in-°F

@Temperature -40.0 - 104 °F
ASTM E 831
SABIC Innovative Plastics LNP THERMOCOMP UF00ASW PPA
LNP* Thermocomp* UF00ASW is a compound based on Polyphthalamide (PPA) containing glass fiber. Characteristics of this grade of Heat Stabilized and Hot Water Moldable.
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP 9H1100C
LNP* Thermocomp* 9H1100C is a High Specific Gravity compound containing proprietary fillers.
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature 50.0 - 200 °C
23.9 µin/in-°F

@Temperature 122 - 392 °F
DIN 53 752
Ensinger TECASINT 1101 Polyimide (PI)
TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel..
CTE, linear, Transverse to Flow 43.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
23.9 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP THERMOCOMP PH0800A PA 6
LNP* THERMOCOMP* PH0800A is a compound based on Nylon 6 resin. Added feature of this material is: High Specific Gravity.