Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP Lubricomp KFL34 Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL34 is a compound based on Acetal Copolymer resin containing Glass Fiber, PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON PFD04 PA 6 LNP* STAT-KON* PFD04 is a compound based on Nylon 6 containing 20% Glass Fiber. Added feature of this grade is: Ellectrically Conductive. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON PFD04ES PA 6 (Europe-Africa-Middle East) LNP* STATKON* PFD04ES is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON PFD04S PA 6 (Europe-Africa-Middle East) LNP* Statkon* PFD04S is a compound based on PA 6 resin containing Glass Fiber, Carbon Powder. Added features include: Electrically Conductive, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON PX93058 PA 6 (Europe-Africa-Middle East) LNP*STATKON*PX93058 is a compound based on PA 6 resin containing Carbon Powder, Glass Fiber. Added features include: Electrically Conductive, Easy Molding, Heat Stabilized. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP STAT-KON RE004 PA 66 (Europe-Africa-Middle East) LNP* Stat-kon* RE004 is a compound based on Nylon 66 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature 23.0 - 60.0 °C |
62.2 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP MFB63 PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFB63 is a compound based on Polypropylene resin containing Glass Bead, Glass Fiber. |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP PPE+PP blend. High Impact, Good Heat Resistance |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C @Temperature -40.0 - 40.0 °C |
62.2 µin/in-°F @Temperature -40.0 - 104 °F |
ASTM E 831 |
SABIC Innovative Plastics NORYL PPX PPX7110 PPE+PP (Asia Pacific) PPE+PP blend. High Impact, Good Heat Resistance |
|||
CTE, linear, Transverse to Flow | 112 µm/m-°C | 62.2 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Heat Stabilized Hydrolysis Resistant Polyamide 66 Zytel 70G25HSLR NC010 is a 25% glass fiber reinforced heat stabilized hydrolysis resistant polyamide 66 resin for injection mol.. |