Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 3.18 mm |
163 °F @Thickness 0.125 in |
Compression Molded, Annealed at 50 deg.C; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Extrusion L4230 Polyvinyl Chloride, Rigid (PVC, Rigid) Extrusion capstock for darker colors. This product is not recommended for horizontal, outdoor applications.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ Vinyl Rigid Molding M4300 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.0 °C @Thickness 3.20 mm |
163 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS Non-chlorinated and non-brominated flame retardant PC+ABS offering balanced flow and impact properties for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.0 °C @Thickness 3.20 mm |
163 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2800 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 72.8 °C @Thickness 6.35 mm |
163 °F @Thickness 0.250 in |
Unannealed; ASTM D648 |
PolyOne Geon™ HTX M6215 Polyvinyl Chloride Alloy (PVC Alloy) It is recommended that the compound pellets be dried for 3 to 4 hours at 150 deg. F.Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.0 °C @Thickness 3.20 mm |
163 °F @Thickness 0.126 in |
Unannealed; ASTM-D648 |
Ineos ABS Lustran® 266 ABS, Transparent Grade Lustran® ABS 266 resin is a clear injection molding grade of ABS (acrylonitrile butadiene styrene). This transparent, general-purpose grade provides clarity and toughness with ease of processing... |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.0 °C @Thickness 3.20 mm |
163 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL N750 PPE+PS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business Equipment applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 73.0 °C @Thickness 3.20 mm |
163 °F @Thickness 0.126 in |
unannealed; ASTM D 648 |
SABIC Innovative Plastics Noryl N750T PPE+HIPS ECO-FLO(tm). ECO conforming, nonhalogenated flame retardant PPE+PS. High flow. Electrical, TV and Business equipment applications.This data was supplied by SABIC-IP for the Americas region. |