Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 75.0 °C | 167 °F | TM R050-25 |
Resinlab® EP1294 Mineral Filled, Flame Retardant Epoxy Syntactic Foam Resinlab™ EP1294 is a two part mineral filled, flame retardant epoxy syntactic foam. It utilizes glass microspheres to reduce cured density and improve machinability. This product will be self-exti.. |
|||
Glass Transition Temp, Tg | 75.0 - 80.0 °C | 167 - 176 °F | Average value: 75.6 °C Grade Count:9 |
Overview of materials for Nylon 46, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | |
Lord Adhesives Thermosetâ„¢ LS 213-9 Unfilled Epoxy Encapsulant Lord LS 213-9 is a one component epoxy coating and impregnating compound featuring low viscosity, good moisture resistance and excellent dielectric properties. Typical applications include transform.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | |
Lucite International Elvacite ® 4026 Acrylic Resin Elvacite® 4026 is a solid acrylic bead resin which has been specially developed for use as a performance enhancing additive in a range of radiation (UV and EB) curable inks and coatings. These en.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | |
Lucite International Elvacite ® 4080 Acrylic Resin Elvacite® 4080 is a medium molecular weight methyl methacrylate copolymer. It is a relatively flexible acrylic resin useful for improving the recoatability and intercoat adhesion of UV wood finis.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Ultimate Tg |
Tra-Con Tra-Bond 216H02 Opaque Black Epoxy Casting Compound TRA-CAST 216H02 is a medium viscosity two-part formulation recommended for general purpose electrical potting and encapsulation applications where the combination of good mechanical thermal and elec.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Ultimate Tg |
Tra-Con Tra-Bond 9070D Filled Epoxy Adhesive TRA-BOND 9070D filled epoxy adhesive exhibits a low coefficient of expansion. Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® 46HF5041LW Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TE250F8 Nylon 46-40% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F3 Nylon 46-15% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200F8 Nylon 46-40% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW200FM33 Nylon 46-30% Glass and Mineral Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW241F12 Nylon 46-60% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW250F6 Nylon 46-30% Glass Reinforced (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW271F6 Nylon 46-30% Glass Reinforced (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW363 Nylon 46 (European Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW371 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Glass Transition Temperature (10°C/min); ISO 11357-1/-2 |
DSM Stanyl® TW441 Nylon 46 (European and Asian Grade) (Dry) Stanyl is a high performance polyamide providing unmatched performance and value across an amazingly broad range of automotive and electronic applications. Stanyl offers:Highest mechanical propertie.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801A NC010A Nylon 66
(Unverified Data**) Zytel® ST801A NC010A is a Super Tough, high performance, polyamide 66 resin. It is partially UV stabilized and when appropriately colored offers limited protection to indirect sunlight exposure.Inf.. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801AHS NC010 Nylon 66
(Unverified Data**) Zytel® ST801AHS NC010 is a Super Tough, high performance polyamide 66 resin. It offers outstanding molding performance in injection molding applications.Information provided by DuPont |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | Average value: 75.0 °C Grade Count:16 |
Overview of materials for Nylon 46, Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 46, Glass Fiber Reinforced". Each property range of values reported is minimum and maximum values .. |
|||
Glass Transition Temp, Tg | 75.0 °C | 167 °F | DAM; 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® ST801 NC010A Nylon 66
(Unverified Data**) Zytel® ST801 is an unreinforced, super tough polyamide 66 for injection molding and extrusion. It offers outstanding break resistance over a wide temperature and humidity range and high productivit.. |
|||
Glass Transition Temp, Tg | 75.0 - 275 °C | 167 - 527 °F | Average value: 178 °C Grade Count:63 |
Overview of materials for Epoxy Molding Compound This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Molding Compound". Each property range of values reported is minimum and maximum values of appropr.. |