Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 170 °C | 338 °F | Wet; DMA |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, 6K 5HS 630-500 Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | Wet; DMA |
Park Electrochemical Nelcote® E-752 Epoxy Prepreg, IM7 Unitape Reinforced Nelcote® E-752 is a toughened, 185°C cure epoxy system designed for demanding structural applications up to 130°C. E-752 offers a good balance of toughness, high service temperature and good mois.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0170 Unsaturated Polyester UP BMC 0170 is a general purpose BMC for electrical applications. Product according to type 801 DIN 16911. The glass content is on a level that combines good mouldability with good strength and stiffne.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0200 Unsaturated Polyester UP BMC 0200 is a standard BMC for general purpose applications. The glass content is on a level that combines good mouldability with good strength and stiffness properties. Even without a specific fire.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0390 Unsaturated Polyester UP BMC 0390 is a low profile DMC/BMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surface qua.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0600 Unsaturated Polyester UP SMC 0600 is a specially formulated SMC for reduced moulding pressure (< 30 bar). The glass level has been selected to combine good mouldability with strength and stiffness. Even without a specific f.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0650 Unsaturated Polyester UP SMC 0650 Low pressure SMC for large panels when moulding force becomes critical. Specific moulding pressure < 20 bar. A Special molding procedure is necessary.Information Provided by Menzolit |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1600 Unsaturated Polyester UP SMC 1600 is a special SMC for sanitary applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The material shows an increased resis.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 0300 Unsaturated Polyester UP BMC 0300 is a low shrink standard material for general-purpose applications, which require a higher level on surface quality and better dimensional stability. The glass content is on a level that co.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2800 Unsaturated Polyester UP BMC 2800 is a high performance BMC for matching the demands of medium and high voltage applications in the electrical field especially in respect of RTI 160+ according to Underwriters Laboratories .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0160 Unsaturated Polyester UP SMC 0160 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0290 Unsaturated Polyester UP SMC 0290 is a specially formulated SMC processable by injection moulding. The gentle production process prevents the fiber from any damage. Parts made of SMC 0290 reach higher levels of strength and.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 2400 Unsaturated Polyester UP SMC 2400 is a SMC with fire retardancy. The glass level has been selected to combine mouldability with strength and stiffness properties. The fire retardancy is especially high, and the material is .. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | ISO 11357-2 |
Menzolit Menzolit® SMC 2500 Unsaturated Polyester UP SMC 2500 is a special SMC for high voltage isolating applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Even without a specific.. |
|||
Glass Transition Temp, Tg | >= 170 °C | >= 338 °F | |
Master Bond EP62-1Med USP Class VI Two Component Epoxy Resin System Master Bond EP62-1Med is a two component epoxy system that has an exceptionally long working life at ambient temperatures and cures rapidly at moderately elevated temperatures. It has a 100 to 10 mi.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | DSC; IPC TM-650 2.4.25 |
Arlon 51N Lead-Free Compatible Epoxy Low-Flow 51N is a non-DICY multifunctional epoxy low-flow prepreg system designed to provide high reliability through lead-free solder operations. The high decomposition temperature and high thermal stabili.. |
|||
Glass Transition Temp, Tg | 170 °C | 338 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N4000-11 Multifunctional Epoxy Laminate and Prepreg The Nelco® N4000-11 is a CAF resistant, high Tg (175º C by DSC) multifunctional epoxy dielectric substrate. This material is formulated to provide the PWB manufacturer and OEM with vastly improved.. |