Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | ISO 11357-1 |
Murtfeldt Murytal® C Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | ISO 11357-1 |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | ISO 11357-1 |
Murtfeldt Murytal® ESD Acetal Copolymer, Conductive Additives make this material conductive. The mechanical properties of the material are retained almost in their entirety. Special Properties:• High rigidity• Excellent ability to regain its form•.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | ISO 11357-1 |
Murtfeldt Murytal® H Acetal Homopolymer In addition to the excellent properties of Murytal® C, Murytal® H is stronger and more rigid with a lower expansion coefficient.Special Properties:• High rigidity• Excellent ability to regain it.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Hytrel® 4069 TPC-ET
(Unverified Data**) Hytrel® 4069 is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like injection.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLCOAT® 163K Thermoplastic Polyurethane Elastomer PEARLCOAT® 163K is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and very good hydrolysis resistance. PE.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | |
Styron XU 36535.00 Formulated SB Performance Features: ENVERSAâ„¢ Cushion Technology, excellent recovery, cushion, excellent acoustic propertiesApplications: Sound DampeningNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | ASTM D3418 |
DuPont Elvaloy® HP4051 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | |
Wanhua Chemical Wanthane® WHT-8280 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | DSC |
Lubrizol ESTANE® 58300 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion with a wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injectio.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | DSC |
Lubrizol ESTANE® 58370 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compoundUses: Extrusion – Wire and cable and general application where flame retardant properties are neededAvailable in Americas, Europe, Middle East, Africa,.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | DSC |
Lubrizol ESTANE® 58630 Ether Based Thermoplastic Polyurethane Features: Good physical properties, hydrolysis resistance, low temperature performance and abrasion along with wide processing window for extrusion and low surface tack.Uses: Blown and flat die/cast.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | DSC |
Lubrizol ESTANE® 58863 Ether Based Thermoplastic Polyurethane Features: Good Elasticity – High melt flow for easy processingUses: Extrusion – Wire and cable, general extrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provi.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Hytrel® 4053FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Hytrel® 4069 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | 10°C/min; ISO 11357-1/-2 |
DuPont Performance Polymers Hytrel® 4056P Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer in Powder FormInformation provided by DuPont Performance Polymers |
|||
Glass Transition Temp, Tg | <= -50.0 °C | <= -58.0 °F | ASTM D3418 |
Arkema Group Pebax® MV1074 Polyether Block Amide |
|||
Glass Transition Temp, Tg | <= -50.0 °C | <= -58.0 °F | ASTM D3418 |
Arkema Group Pebax® MV1657 Polyether Block Amide |
|||
Glass Transition Temp, Tg | <= -50.0 °C | <= -58.0 °F | Cured property; Perkin Elmer TM-2 |
Aptek 2313-PMF Hybrid Epoxy Adhesive Snap-cure, silver-filled; long pot-life/stable viscosity-excellent for robotics. Thermal shock resistant.Production-oriented, snap-cure technology for surface mount applications-allows cure during s.. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | 10°C/min |
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Dry) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |
|||
Glass Transition Temp, Tg | -50.0 °C | -58.0 °F | DSC |
Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection.. |