| Physical Properties | Metric | English | Comments | 
|---|---|---|---|
| Density | 1.07 g/cc | 0.0387 lb/in³ | ISO R1183; ASTM D792 | 
| Moisture Absorption at Equilibrium | 1.4 % | 1.4 % | at equilibrium at 50% RH; ASTM D3418 | 
| 1.4 % | 1.4 % | at equilibrium at 50% RH; ASTM D3418 | 
| Mechanical Properties | Metric | English | Comments | 
|---|---|---|---|
| Elongation at Break | >= 700 % | >= 700 % | ISO R527 | 
| Flexural Modulus | 0.0900 GPa | 13.1 ksi | ISO 178; ASTM D790 | 
| Izod Impact, Notched | NB | NB | ISO 180/ASTM D256 | 
| Thermal Properties | Metric | English | Comments | 
|---|---|---|---|
| Melting Point | 158 °C | 316 °F | ASTM D3418 | 
| Glass Transition Temp, Tg | <= -50.0 °C | <= -58.0 °F | ASTM D3418 | 
| Optical Properties | Metric | English | Comments | 
|---|---|---|---|
| Refractive Index | 1.502 | 1.502 | ISO 489 | 
| Electrical Properties | Metric | English | Comments | 
|---|---|---|---|
| Electrical Resistivity | 2.50e+8 ohm-cm | 2.50e+8 ohm-cm | ASTM D257 | 
| Surface Resistance | 3.00e+8 ohm | 3.00e+8 ohm | ASTM D257 |