Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® E51HSB NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized High Viscosity Polyamide 66 Zytel E51HSB NC010 is a high molecular weight heat stabilized polyamide 66 resin for injection molding and extrusion.Information provided by .. |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® EFE1068 NC010T Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel EFE1068 NC010T is a lubricated polyamide 66 for injection molding. It has excellent flow characteristics and was developed for fast production cycles and high producti.. |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® FG101L NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66 with Developed for Food Contact ApplicationsZytel FG101L NC010 is a lubricated polyamide 66 resin for injection molding. It has been developed for consideration into applic.. |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® FG42A NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact ApplicationsZytel FG42A NC010 is a high viscosity polyamide 66 resin for injection molding and extrusion. It has been develop.. |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® FG42L NC010 Nylon 66
(Unverified Data**) Unreinforced High Viscosity Polyamide 66 with Developed for Food Contact Applications Information provided by DuPont Performance Polymers |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® 103FHS NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHS NC010 is a heat stabilized internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivi.. |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® 103FHSA NC010 Nylon 66
(Unverified Data**) Unreinforced Heat Stabilized Polyamide 66 Zytel 103FHSA NC010 is a heat stabilized lubricated polyamide 66 for injection molding.Information provided by DuPont Performance Polymers |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® 101 NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101 NC010 is a general purpose polyamide 66 resin for injection molding and extrusion.Information provided by DuPont Performance Polymers |
|||
Specific Heat Capacity | 2.79 J/g-°C | 0.667 BTU/lb-°F | |
DuPont Performance Polymers Zytel® 101F NC010 Nylon 66
(Unverified Data**) Unreinforced Polyamide 66Zytel 101F NC010 is an internally lubricated polyamide 66 resin for injection molding. It was developed for fast cycles and high productivity.Information provided by DuPont .. |