Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | DSC |
Eastman Heatwave CF746 Polymer
(discontinued **) Heatwave is a clear, reheat enhanced, PET polyester designed for heatset containers containing a UV light protection package chemically bound to the backbone of the polymer. Pellets are 2.5 mm (0.1 .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman Aqua 18696 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Containers made from 186.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman Aqua 20837 PET
(discontinued **) Voridian Aqua thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. Voridian Aqua polymer 20.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 7352 PET
(discontinued **) VORIDIAN PET thermoplastic polyesters are condensation polymers produced by a continuous melt-phase polymerization process followed by a solid-state polymerization process. VORIDIAN PET polyester 73.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman CM01 PET
(discontinued **) Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman GP800 PET
(discontinued **) Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | IES 1006 |
Polycasa LENTICULAR PETG Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advert.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0180 Unsaturated Polyester UP BMC 0180 is a general purpose BMC for electrical applications. Product according to type 803 DIN 16911. The glass content is on a level that combines good mould ability with good strength and stiffn.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0800 Unsaturated Polyester UP BMC 0800 is a special SMC for applications within household and kitchenware. The glass level has been selected to combine good mould ability with good strength and stiffness properties. The product .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0170 Unsaturated Polyester UP SMC 0170 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0200 Unsaturated Polyester UP SMC 0200 is a general purpose SMC for a wide range of applications. Typically, it is used as housings, covers and functional components in mechanical engineering. The flammability meets the demands .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0390 Unsaturated Polyester UP SMC 0390 is a standard low profile SMC. Because of its low shrinkage, the material shows good surface quality as well as very low warpage. The product is suitable for applications if a better surfac.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0410 Unsaturated Polyester UP SMC 0410 is a Premium Class-A SMC for on-line painted exterior body applications on cars developed with CCC technology. These compounds mould to parts with excellent surface quality for on-line pain.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fi.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP SMC 1000 is a special SMC for hydrolysis resistant applications. The glass level has been selected to combine good mouldability with good strength and stiffness properties. Typical applications are .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1400 Unsaturated Polyester UP SMC 1400 is a special SMC being used in the environment of a combustion engine. The glass level has been selected to combine good mouldability with good stiffness and strength properties. The produc.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 1650 Unsaturated Polyester UP SMC 1650 is a specially designed anti-microbial polyester moulding compound which incorporates a "germ killer" . It has been tested and found to be compliant for resistance to fungal defacement in .. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 0190 Unsaturated Polyester UP BMC 0190 is a general purpose BMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The flammability me.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0150 Unsaturated Polyester UP SMC 0150 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0190 Unsaturated Polyester UP SMC 0190 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Menzolit Menzolit® SMC 0300 Unsaturated Polyester UP SMC 0300 is a low shrink standard SMC providing improved surface quality, reduced shrinkage and warpage. Typical fields of applications are mechanical engineering and electrical industry, where impr.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Haveg 41NA Phenolic; Silicate Filled A proprietary thermoset plastic consisting of a phenol-formaldehyde resin and non-asbestos silicate fillers. |
|||
Specific Heat Capacity | 1.10 J/g-°C @Temperature 100 - 200 °C |
0.263 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec 665 Steatite, MgO•SiO2 Steatites used in place of aluminas are a cost-effective way to meet performance requirements. They are easier to form and fire at lower temperatures. 665 L533C has low dielectric loss. It makes exc.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | |
Hippe PET Polyethylene Terephthalate Linear, saturated polyesters are thermoplastics which are used where good dimensional accuracy, high creep resistance and good sliding and wear behavior are required. Partially crystallized PET pos.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-3283 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3283 is a non-conductive, thermally and chemically stable liquid ideal for use in single phase heat transfer applications, especially in the electronics and semiconductor.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | Liquid |
3M Fluorinert™ FC-3284 Electronic Liquid 3M™ Fluorinert™ Liquid FC-3284 is a non-conductive, thermally and chemically stable fluid ideal for use in single and two phase heat transfer fluid applications, such as semiconductor package test.. |
|||
Specific Heat Capacity | 1.10 J/g-°C | 0.263 BTU/lb-°F | ASTM E1269 |
Eastman 9921W PET Film
(discontinued **) Voridian PET 9921W is a copolymer PET. Typical applications include containers for automotive parts, household products, and pharmaceutical and food packaging. Voridian PET thermoplastic polyesters .. |