Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Parkway Products Thixomolded® AM50A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | ASTM E1461 |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-35 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | Average value: 1.05 J/g-°C Grade Count:8 |
Overview of materials for Polyperfluoroalkoxyethylene (PFA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Polyperfluoroalkoxyethylene, Molded/Extruded". Each property range of values reported is minimum and max.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 100 °C |
0.250 BTU/lb-°F @Temperature 212 °F |
|
Kaiser 7068 T6, T651 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 100 °C |
0.250 BTU/lb-°F @Temperature 212 °F |
|
Kaiser 7068 T6, T6511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Specific Heat Capacity | 1.05 J/g-°C @Temperature 100 °C |
0.250 BTU/lb-°F @Temperature 212 °F |
|
Kaiser 7068 T76, T76511 Rod & Bar Alloy 7068 offers some of the highest strength mechanical properties available in an extruded product. Intended for aerospace, ordnance and light weight recreational applications where extremely hig.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics AL-30 Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALBF Alumina Bulk Fiber Alumina Bulk Fiber Type ALBF consists of long aluminum oxide fibers suited for the vacuum forming of low density shapes. The high alpha alumina content and addition of a grain growth inhibitor give .. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALBF-1 Alumina Bulk Fiber Type ALBF-1 Alumina Bulk Fiber is a specially cleaned alumina fiber with relatively short fiber lengths. It is suitable for use in vacuum forming of high density rigid boards & shapes, in the reinfo.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALC Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ECO-20AA Alumina Insulation ECO-20AA is most commonly utilized as hotface insulation in furnaces with hydrogen rich atmospheres such as bright annealing furnaces.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics SALI Alumina Insulation SALI has been serving 1700°C low mass furnace users longer than any other alumina fiber board available today. SALI is a premium grade rigid fiber board with superior hot strength.Information provi.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics SALI-2 Alumina Insulation SALI-2 is a premium grade rigid insulation board used as hotface insulation or a precision machined furnace fixtures.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-15 Alumina Boards, Discs & Cylinders Insulation Zircar alumina insulation Type M Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with with silica binders in BusterM that form a thermal shock resistant mullite.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Zirconia Buster M-35 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics Alumina Mat A layered, low density flexible mat made of 100% polycrystalline alumina fiber (non-RCF) designed for use to temperatures as high as 1650°C (3002°F). Shot free low density mat used as fill between.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-45 Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Enviro Tech International EnSolv® Ionic n-Propyl Bromide Vapor Degreasing Solvent EnSolv-Ionic is the perfect direct replacement for TCE, Perchloroethylene, 1,1,1-Trichloroethane, HCFC-141b, Freon and other hazardous or discontinued vapor degreasing, ultrasonic and manual cleanin.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Parkway Products Thixomolded® AZ91D Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ALCAA Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-15 Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
Specific Heat Capacity | 1.05 J/g-°C | 0.250 BTU/lb-°F | |
Parkway Products Thixomolded® AM60A Magnesium Thixomolding® is a fabrication technique, similar to injection molding, that uses magnesium alloys as the “resin” instead of plastic. Solid magnesium alloy pellets are fed into the machine, heate.. |