Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4429 Cr-Ni-Mo Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto), cold rolled strip/sheet and rod forms. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4436 Cr-Ni-Mo Austenitic Stainless Steel General purpose steel with excellent corrosion resistance, particularly in the presence of halides.Applications: FiltersBraiding for hydraulic hosesShaftsFastenersMarine componentsAvailable in hot r.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4501 Duplex Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | RT |
Outokumpu 4571 Cr-Ni-Mo Austenitic Stainless Steel Very good corrosion resistance, weldable, and resistant to sensitization.Available in hot rolled plate (Quarto), hot rolled strip/sheet (CPP), cold rolled strip/sheet, cold rolled narrow strip, bar,.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 20.0 - 100 °C |
0.120 BTU/lb-°F @Temperature 68.0 - 212 °F |
|
Industeel CLC 17.13.3 LN Nitrogen Containing 18Cr-10Ni-2Mo Austenitic Stainless Steel Description: CLC 17-13-3LN is a nitrogen alloyed austenitic stainless steel with Mo additions. Its low carbon content avoids intergranular corrosion, even on welded pieces without an ulterior water .. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 20.0 °C |
0.120 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 309 23% Cr - 13% Ni Heat Resistant Stainless Steel Description: CLI SIRIUS 309 grade is a fully austenitic stainless steel containing 23% Cr, and 13% Ni additions. The alloy is well known for its multi-purpose high temperature corrosion resistance b.. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 500 °C |
0.120 BTU/lb-°F @Temperature 932 °F |
|
Haynes 188 alloy, 40% cold reduction, 3.2 mm thick sheet Excellent high temperature strength and very good resistance to oxidizing environments up to 1095°C for prolonged exposure, and excellent resistance to sulfate deposit hot corrosion. Readily fabr.. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 20.0 °C |
0.120 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel SIRIUS 800 Heat Resistant Alloy Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at t.. |
|||
Specific Heat Capacity | 0.503 J/g-°C @Temperature 400 °C |
0.120 BTU/lb-°F @Temperature 752 °F |
|
Haynes 625 alloy, plate after 4000 hours at 760°C (1400°F) Cb and Ta content 3.7% combined. Excellent strength up to 816°C, good oxidation resistance and aqueous corrosion, excellent forming and welding characteristics. Applications include a variety of .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Special Metals INCOLOY® 25-6M0 Super Austenitic Stainless Steel (UNS N08926) Data provided by the manufacturer, Special Metals. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 100 - 200 °C |
0.120 BTU/lb-°F @Temperature 212 - 392 °F |
DINV ENV 821-3 |
CeramTec Sikor® E Cordierite Cordierites have low coefficients of thermal expansion and excellent resistance to thermal shock. They offer a range of thermal expansion, mechanical strength, and porosity criteria. They excel as c.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Annealed Sheet/Plate & Billet/Bar Low Cost, Multipurpose Alloy. Tensile property data below for Annealed Sheet/Plate & Billet/Bar.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, but wit.. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 321 Chromium-Nickel Steel Crucible 321 is a non-hardenable, low carbon austenitic chromium-nickel steel which is particularly adaptable for parts fabricated by welding without postweld annealing for use at temperatures betwe.. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
Crucible Steel 304L Chromium-Nickel Steel Crucible 304L is a non-hardenable, low carbon austenitic chromium-nickel steel designed for special applications. It is particularly suitable for applications requiring welding operations where it i.. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
AK Steel 309S Austenitic Stainless steel AK Steel 309S provides excellent corrosion resistance and heat resistance plus good strength at room and elevated temperatures. The alloy is non-magnetic as annealed and becomes slightly magnetic w.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Carpenter 20Cb-3® Stainless Steel Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Carpenter 20Cb-3® Stainless Steel, Bar, Annealed at 1750°F (955°C) then Water Quenched Data provided by Carpenter Technology Corporation.20Cb-3® is an austenitic stainless steel possessing excellent resistance to hot sulfuric acid and many other aggressive environments which would re.. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum 310H Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum 310Si Austenitic Stainless Steel Characteristics: comparable corrosion resistance, superior resistance to oxidation, and the retention of a larger fraction of room temperature strength than common austenitic alloys. Good creep defo.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum AL 20™ Plate Specialty Steel The N08020 alloy has been available for many years and has found applications in many environments, such as in chlorides and in sulfuric and sulfurous acids.Although AL 20 alloy was developed for im.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 302, 20% Cold Rolled (UNS S30200) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304L, 50% Cold Rolled (UNS S30403) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, Annealed (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.502 J/g-°C @Temperature 0.000 - 100 °C |
0.120 BTU/lb-°F @Temperature 32.0 - 212 °F |
|
ATI Allegheny Ludlum Stainless Steel Type 201, 60% Cold Work (UNS S20100) Allegheny Ludlum Type 201 and 201L have the greatest tonnage of the Cr-Ni-Mn steels (200 series). Type 201 provides advantages over the 18-8 grades in certain applications. Lower cost manganese an.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 304, 0% Cold Rolled (UNS S30400) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
ATI Allegheny Ludlum Stainless Steel Chromium-Nickel Type 305, 30% Cold Rolled (UNS S30500) This alloy is one of the most familiar and most frequently used alloy in the stainless steel family. It may be best used in applications where the following properties are important: resistance to .. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
TIMET TIMETAL® 62S Titanium Alloy (Ti-6Al-2Fe-0.1Si); Alpha-Beta Forged, RA Low Cost, Multipurpose Alloy. Tensile/toughness property data below for Alpha-Beta Forged, RA material.Features: Properties and processing characteristics equivalent to or better than TIMETAL 6-4, .. |
|||
Specific Heat Capacity | 0.500 J/g-°C @Temperature 20.0 °C |
0.120 BTU/lb-°F @Temperature 68.0 °F |
|
Industeel UREA 316L Modified 316L Mod Low Si, High Mo Stainless Steel for Urea Plants Description: UREA 316L Modified grade has been specially developed for Urea plant applications. It is a 316L modified stainless steel with extra-low silicon content and substantial higher molybdenum.. |
|||
Specific Heat Capacity | 0.500 J/g-°C | 0.120 BTU/lb-°F | |
Special Metals INCOLOY® Alloy 020 A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellen.. |