Thermal Properties Metric English Comments
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total 3802 B HDPE, cable, sheet, pipe, injection molding
FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total 3802 Blue MDPE pipe, injection molding
FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total 3802 YCF MDPE pipe grade
FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total HP 401 MDPE, pipe, cable, sheet
FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total Xsene® XS10 B HDPE, pipe, injection molding
FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS10 B is a high performance black compound speci..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total Xsene® XS10 H HDPE, pipe, injection molding
FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound..
Specific Heat Capacity 2.60 J/g-°C
0.621 BTU/lb-°F
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66  (Unverified Data**)
Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total Lacqtene® 2001 TBK 46 HDPE pipe  (discontinued **)
LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and ..
Specific Heat Capacity 2.60 - 2.60 J/g-°C

@Temperature 150 - 150 °C
0.621 - 0.621 BTU/lb-°F

@Temperature 302 - 302 °F
Average value: 2.60 J/g-°C Grade Count:8
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade
This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max..
Specific Heat Capacity 2.60 J/g-°C

@Temperature 150 °C
0.621 BTU/lb-°F

@Temperature 302 °F
DSC
Total Xsene® XS10 Orange YCF HDPE, pipe
FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance ..