Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 243 °C | 469 °F | ISO 3146 |
PolyOne Bergamid™ AB700 UF Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Melting Point | 243 °C | 469 °F | ISO 3146 |
PolyOne Bergamid™ AB700 UF SO Polyamide 66/6 Copolymer (Nylon 66/6) Information provided by PolyOne |
|||
Melting Point | 243 °C | 469 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman Aqua WA314 PET
(discontinued **) Voridian Aqua PET WA314 is a polyethylene terephthalate resin designed for single-serve bottled water applications. WA314 has an intrinsic viscosity of 0.76 and provides sparkling clarity and fast i.. |
|||
Melting Point | 243 °C | 469 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman A12 PET
(discontinued **) Voridian Polymer A12 is currently produced to Eastman`s specifications and quality requirements by several resin manufacturers located in the Asis Pacific Region. Voridian Polymer A12 is available i.. |
|||
Melting Point | 243 °C | 469 °F | Crystalline Peak Melting Point; ASTM D3418 |
Eastman CB11E PET
(discontinued **) VORIDIAN PET CB11E is designed specifically for the carbonated soft drink (CSD) and other beverage markets in the European market area. The polymer delivers faster, more efficient processing and bet.. |
|||
Melting Point | 243 °C | 469 °F | |
Eastman Eastapak 9921 PET ISO data as provided by the manufacturer, Eastman Chemical |
|||
Melting Point | 243 - 249 °C | 469 - 480 °F | |
Ex-Tech Plastics VersaTech™ PET Ex-Alloy 3400, 100% Post Consumer FDA, RPET Extruded Sheet Delivering all the qualities of PET, this sheet is developed using post consumer material, allowing the packaging to carry marketing reference terms such as sustainability, green and recycled.Charac.. |
|||
Melting Point | <= 243 °C | <= 469 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil Exceed™ 2018HA Metallocene Polyethylene Resin (European Grade) Product Description: Exceed 2018HA is a metallocene Catalyzed ethylene-hexene copolymer. Films made from Exceed 2018HA have outstanding tensile, impact strength, and puncture. These superior strengt.. |
|||
Melting Point | 243 °C | 469 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® C 4800 B66A PET Product Description: Laser+® 4800 (B66A) is a unique copolymer particularly suited for use in the custom PET reusable, bulk container applications where clarity in thicker performs is desired. It i.. |
|||
Melting Point | 243 °C | 469 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® C 9000 (B64A) PET Product Description: Laser+® 9000 (B64A) is a unique copolymer particularly suited for use in the custom PET container applications where clarity and neutral color are desired. It is a medium intri.. |
|||
Melting Point | 243 °C | 469 °F | nominal; DAK-QAR-SOP-0016 |
DAK Americas Laser+® HS D59A PET Product Description: Laser+® HS (D59A) polyethylene terephthalate (PET) resin is designed for conversion to PET packaging by injection stretch blow-molding using commercial heat-set technology.Typi.. |
|||
Melting Point | <= 243 °C | <= 469 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 152BW Low Density Polyethylene Resin Product Description: LD 152BW is an LDPE grade offering an excellent combination of optical properties and stiffness. The 2.2 MI makes it ideal for blowing thicker films.Availability: Africa & Middl.. |
|||
Melting Point | 243 °C | 469 °F | DIN 53765 |
BASF Ultramid® C3U BK 23079 PA6/66 FR (Conditioned) Description: Injection-molding grade with improved flame retardance (free from halogens and phosphorus), used e.g. for impact resistant electrically insulating parts such as contact bases and plug c.. |
|||
Melting Point | 243 °C | 469 °F | DIN 53765 |
BASF Ultramid® C3U PA66/6 (Conditioned) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 Nylon 66/6 Unreinforced, medium viscosityInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 R Nylon 66/6 High impact resistanceInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 V30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 V40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | 10 K/min |
BASF Ultramid® C3U BK23079 PA66/6 (Dry) Ultramid C3U BK23079 is an injection molding, general purpose PA66/6, pigmented black grade with improved flame retardance. |
|||
Melting Point | 243 °C | 469 °F | ASTM Test |
BASF Ultramid® C3U BK23079 PA66/6 (Dry) Ultramid C3U BK23079 is an injection molding, general purpose PA66/6, pigmented black grade with improved flame retardance. |
|||
Melting Point | 243 °C | 469 °F | DIN 53765 |
BASF Ultramid® C3U PA66/6 (Dry) Ultramid C3U is an injection molding, general purpose PA66/6 grade with improved flame retardance. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 M20 V10 Nylon 66/6, Glass/Mineral Filled Mixed products with improved stiffness and good dimensional stability, low warpage.Information provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 V15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 V20 Nylon 66/6, 20% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 ZV15 Nylon 66/6, 15% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 ZV20 Nylon 66/6, 20% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 ZV30 Nylon 66/6, 30% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |
|||
Melting Point | 243 °C | 469 °F | ISO 3146/C2 |
Addiplast Addinyl C2 ZV40 Nylon 66/6, 40% Glass Filled Glass fiber reinforced, increased thermal aging stabilityInformation provided by Addiplast. |