Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 230 °C | 446 °F | |
Oceanchem Group 2,4,6-Tris (2,4,6-tribromophenoxy)-1,3,5-triazine (FR245 Molecular Formula: C21H6Br9N3O3Cas No.: 25713-60-4Use: FR245 a brominated cyanurate is a proprietary, additive flame retardant. The comination of aromatic bromine and cyanurate provides high FR eff.. |
|||
Melting Point | 230 °C | 446 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasalac 3P-H9000B ABS/PC Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Melting Point | 230 °C | 446 °F | ISO 11357-3 |
Pasargad Polymer Peyvand Pasalac 3P-H9000W ABS/PC Form: PelletsProcessing Method: Injection MoldingUses: Automotive Application Furniture Appliance Components Automotive Exterior PartsAutomotive Interior PartsInformation provided by Pasargad Poly.. |
|||
Melting Point | >= 230 °C | >= 446 °F | |
Pau Tai Barium stearate, Monomer Stabilizer Excellent effect if used with cadmium, zinc, lead. Excellent lubricity and electrical insulation. Resistance to sulfide staining.Applications: Applicable to hard, soft common adhesive plaster, rubbe.. |
|||
Melting Point | 230 °C | 446 °F | |
Solvay Specialty Polymers Ixef® BXT-2000/0203 Polyarylamide (PARA)
(Unverified Data**) Ixef BXT-2000/0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef BXT-2000/0203 resin can be successfully extruded into.. |
|||
Melting Point | 230 - 246 °C | 446 - 475 °F | Limits; M2E-73-002 |
Indorama Ventures Mexico Polyclear™ Preserve 2201 PET Resin Description: La resina Polyclear® Preserve PET 2201 de Arteva Specialties, es un copolimero para empaque con una viscosidad intrinseca de 0.84 dl/g y esta disenada para ofrecer un redimiento supe.. |
|||
Melting Point | 230 - 250 °C | 446 - 482 °F | |
Johnson Matthey JM 97C Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 230 - 235 °C | 446 - 455 °F | |
Johnson Matthey JM 99C Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Melting Point | 230 °C | 446 °F | DSC |
Solvay Specialty Polymers Ixef® BXT 2000-0203 Polyarylamide (PARA) Ixef® BXT 2000-0203 resin was developed specifically for extrusion and blow-molding processes. Unlike grades targeted for injection molding, Ixef® BXT 2000-0203 resin can be successfully extru.. |
|||
Melting Point | 230 °C | 446 °F | |
Solvay RHODAQUAT® M-242B/99 Surfactant Description: Rhodaquat® M-242B/99 is high purity cationic surfactant A free flowing crystalline powder has unique property of static and tangling elimination, imparting soft and elegant feel to h.. |
|||
Melting Point | 230 °C | 446 °F | |
Tisan TISARBON® 10% Glass Fiber Reinforced Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Melting Point | 230 °C | 446 °F | |
Tisan TISARBON® Flame Retardant (V0) Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Melting Point | 230 °C | 446 °F | |
Tisan TISARBON® UNR Polycarbonate TISARBON has a wide area of application in construction, building auxiliary materials, electric/electronic, lighting equipment, home appliances, automotive, telecommunication and health products ind.. |
|||
Melting Point | 230 - 282 °C | 446 - 540 °F | |
Zeus ETFE Tubing ETFE (Ethylenetetrafluoroethylene), a copolymer of ethylene and tetrafluoroethylene, is used in applications requiring excellent impact, abrasion and stress cracking resistance. This polymer possess.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 051.LQ Low Density Polyethylene Resin Product Description: LD 051.LQ blown film resin is a fractional melt index grade designed for demanding heavy duty film applications, and combines excellent strength properties with outstanding proc.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 100.BW Low Density Polyethylene Resin Product Description: LD 100.BW is a LDPE grade, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.Ava.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 100AC Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 100BR Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin Product Description: LD 100 series are LDPE grades, offering a good balance of optical and mechanical properties. Several additive packages are available according to the required surface properties.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 100BW Low Density Polyethylene Resin (European Grade) Product Description: LD 100BW is a LDPE containing low antioxidants suitable for the production of LV and MV crosslinked insulation using the 1-step or 2-step silane technology. Through in-house com.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 101BA Wire & Cable Low Density Polyethylene Resin Product Description: LD 101BA Wire & Cable is anon-stabilized LDPE, designed for the production of Medium/High Voltage insulation using the direct peroxide addition. For cleanliness reasons, the mat.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 185BW Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 185GE Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 185JD Low Density Polyethylene Resin (European Grade) Product Description: LD 185 series offer good optical properties and sealing characteristics. LD 185 is manufactured with narrow specifications to suit the high consistency requirements of laminatio.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 503.LP Low Density Polyethylene Resin Product Description: LD 503.LP is a LDPE homopolymer that is suitable for use in molding, extrusion, compounding and foam applications.Availability: Latin America, North America and South AmericaAdd.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 506.07 Low Density Polyethylene Resin Product Description: LD 506.07 is a high flow, LDPE homopolymer designed to provide good processability. It is suitable for use in making color concentrates and injection molded articles.Availabilit.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 516.LN Low Density Polyethylene Resin Product Description: LD 516.LN is a medium MI, low density polyethylene resin designed for use in color concentrates and masterbatches where its flow properties ensure improved processability and un.. |
|||
Melting Point | <= 230 °C | <= 446 °F | Peak Melting Point; ExxonMobil method |
ExxonMobil LDPE LD 617.LN Low Density Polyethylene Resin Product Description: LD 617.LN is a high flow, low density polyethylene homopolymer resin designed to provide excellent processability, flexibility and surface appearance. This multipurpose resin is.. |
|||
Melting Point | 230 °C | 446 °F | HG/T2235 |
Beijing Evergrow Resources MoS2 Filled Nylon Information provided by Beijing Evergrow Resources. |