Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 160 °C | 320 °F | STN EN 11357-1 |
Plastcom PLASTALEN® PC 69 T 10 003 Polypropylene reinforced with mineral filler Modified PP copolymer for injection molding with the content of 10% mineral filler. Application in all automotive industry. Delivered in black.Information Provided by Plastcom spol. s r.o. |
|||
Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PC 51 C 30 Polypropylene Homopolymer and Copolymer, 30% Micronized Talc FeaturesModified homopolymer and copolymer PP for injection moulding with the content of 30% micronized, chemically modified talc. Increased strength, rigidity and thermal application up to 120°C... |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 78 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. Stable towards detergents. General application in all industry branches.. |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | ASTM D3418 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Melting Point | 160 °C | 320 °F | ASTM D3418 |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Melting Point | 160 °C | 320 °F | STN EN 11357-1 |
Plastcom PLASTALEN® PH 52 T 20 Polypropylene reinforced with mineral filler PP homopolymer for injection molding with the content of 20 % mineral filler, heat stabilized. Application in automotive industry. Delivered in black grade.Information Provided by Plastcom spol. s r.. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 91 T 40 PP, 40% mineral filling FeaturesModified homopolymer PP for injection moulding with the content of 40% microground, floated, chemically modified talc. General application in all industry branches - packing material, garden.. |
|||
Melting Point | 160 °C | 320 °F | ASTM D3418 |
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride
(discontinued **) Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a.. |
|||
Melting Point | 160 - 175 °C | 320 - 347 °F | Huntsman/TMA |
Huntsman IROGRAN® A 78 E 4588 Polyester-Based TPU-High Performance Grade High Hydrolysis resistance and good crystallinity. Suggested for injection molding.Information provided by Huntsman |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 P 4637 TPU-Polyether Excellent resistance to hydrolysis and microbial attack. Suggested for injection molding and extrusion.Information provided by Huntsman |
|||
Melting Point | 160 - 190 °C | 320 - 374 °F | Huntsman/TMA |
Huntsman IROGRAN® A 92 E 4694 Polyester-Based TPU-Injection Extrusion Grade Introduction: IROGRAN A 92 E 4694 is a thermoplastic special- polyester-polyurethane for injection moulding and extrusion applications. Additional characteristics of the product are flexibility and .. |
|||
Melting Point | 160 °C | 320 °F | |
ScanTube PVDF Tubing Information provided by ScanTube, Inc. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
Total PPC 5724 Polypropylene, Extra High Impact Copolymer ATOFINA 5724 is characterized by a high fluidity offering a combination of processing and excellent impact properties in applications ranging from industrial to household.ApplicationATOFINA 5724 has.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | ATOFINA Method |
Total PPC 4944WZ Polypropylene, Impact Copolymer ATOFINA 4944 polypropylene is a nucleated and controlled rheology impact copolymer. 4944WZ is characterized by improved stiffness and impact resistance, as well as low shrinkage and low warpage. I.. |
|||
Melting Point | 160 °C | 320 °F | ISO 3146 |
Chengdu Polyster H3030 Thermoplastic Polyether-ester Elastomer (TPEE) Information provided by Chengdu Polyster Co., Ltd. |
|||
Melting Point | 160 °C | 320 °F | |
Daikin NEOFLON RP-4020 EFEP Pellets NEOFLON EFEP is an ETFE based fluoropolymer combining the excellent physical properties derived from ETFE together with a low processing temperature that is more compatible with conventional thermop.. |
|||
Melting Point | 160 - 165 °C | 320 - 329 °F | [10 K/min], ISO 11357 |
Eurotec® Tecolen® CP10 GR50 NL PPCP, 50% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Melting Point | 160 °C | 320 °F | (Dry) |
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Melting Point | 160 - 174 °C | 320 - 345 °F | |
AIM 70In/30Pb Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Melting Point | 160 - 170 °C | 320 - 338 °F | |
BCC Products BC 100 Thick Cyanoacrylate Adhesive BC100 Thick is the slow and thickest member of the BCC Products line of cyanoacrylate adhesive. Excellent for gap filling the BC100 Thick has a 30 second fixture time allowing for the material to f.. |
|||
Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 51 T 15 Polypropylene Homopolymer, 15% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 15% mineral filler. Increased rigidity, strength and thermal use up to 130°C. Decreased shrinkage. General application .. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 61 GB 30 PP, 30% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 91 N Polypropylene Homopolymer FeaturesModified homopolymer PP for injection moulding. General use in all industry branches - packing material, garden flower-pots, toys, furniture industry, hinges, fasteners, clamps, office chai.. |
|||
Melting Point | 160 °C | 320 °F | ASTM D789 |
Adell RR-14 Copolymer Polypropylene, 20% Glass Reinforced Data provided by Adell Plastics, Inc. |
|||
Melting Point | 160 °C | 320 °F | ASTM D789 |
Adell RA-16 Copolymer Polypropylene, 30% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 160 °C | 320 °F | ASTM D789 |
Adell RA-18 Copolymer Polypropylene, 40% Talc Filled Data provided by Adell Plastics, Inc. |
|||
Melting Point | 160 °C | 320 °F | DSC; STN EN ISO 3146 |
Plastcom SLOVALEN PH 51 T 10 Polypropylene Homopolymer, 10% Mineral Filled FeaturesModified homopolymer PP for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal use up to 120°C. Decreased shrinkage. General application .. |
|||
Melting Point | 160 °C | 320 °F | |
Plastcom SLOVALEN PH 69 GF 40 PP, 40% glass fibre, mod. of mech. properties FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 40% glass fibre, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |
|||
Melting Point | 160 - 167 °C | 320 - 333 °F | Average value: 164 °C Grade Count:18 |
Overview of materials for Polypropylene, Long Glass Fiber 50% This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Long Glass Fiber 50%". Specific grades with glass content between 45% and 54% are include.. |
|||
Melting Point | 160 °C | 320 °F | DSC; Dow Method |
Braskem INSPIRE™ 222 Performance Polypropylene Polymer INSPIRE™ 222 Performance Polymer is intended for use in extrusion and thermoforming processes. It is especially suited in applications requiring excellent clarity and good stiffness.Contains a nuc.. |