Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 131 °C | 268 °F | Petromont |
Petromont 2001 High Density Polyethylene Resin Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion an.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total Finathene® 3344N Natural HDPE pipe grade
(discontinued **) Applications: industrial and mining gas distribution, potable water, sewer and sewer relining, gas and oil gathering, fiber optic innerduct, general pipe reliningInformation provided provided by To.. |
|||
Melting Point | 131 °C | 268 °F | ISO 3146 |
Total Lacqtene® 2004 TN 52 HDPE pipe
(discontinued **) LACQTENE® 2004 TN 52 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2004 TN 52 is best processed between 190 and 230°C.Informa.. |
|||
Melting Point | 131 °C | 268 °F | |
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Melting Point | 131 - 170 °C | 268 - 338 °F | |
Indium Corp. Indalloy 99 Bismuth-Lead-Tin Solder Alloy Information Provided by Indium Corporation |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Global J-1600 High Density Polyethylene Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation. |
|||
Melting Point | 131 °C | 268 °F | 10°C/min; ASTM D3418 |
LG Chemical SEETEC PM360 HDPE Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
Lushan L-5R (HC) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5604F High Density Polyethylene Film Key Characteristics:High tensile strengthHigh dart impactHigh stiffnessLow gel contentGood moisture barrierRecommended Applications: Films for shopping bag, T-shirt bag, garbage bag, liner bagInfor.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5814J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total HDPE XT25N High Density Polyethylene, Pipe Resin Polyethylene: High molecular weight, bimodal pipe resin. PPI TR4 designation PE4710 /PE100 for demanding installations. Every batch certified to meet 2500 hrs PENT according to ASTM F1473.Charact.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357 |
Total Lumicene® mPE M5220 M Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M5220M is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, stress-cr.. |
|||
Melting Point | 131 °C | 268 °F | ISO 11357 |
Total Lumicene® mPE M5220 Metallocene High Density Polyethylene This product is a Total Ecosolutions grade.Lumicene® mPE M 5220 is a High Density Polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity an.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E924 Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924 is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristics.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E924ND Film HDPE High Molecular Weight High Density Polyethylene (HMW-HDPE) for Film Extrusion Formolene® E924ND is a bi-modal HMW-HDPE resin designed for high dart impact strength and good processing characteristi.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418, ISO 3146 |
DuPont™ Fusabond® E265 Polymer Modifier DuPont™ Fusabond® E265 is an anhydride modified high density polyethylene. Used as a polymer modifier |
|||
Melting Point | 131 °C | 268 °F | Equate Test Method |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow DMDA-8907 NT 7 High Density Polyethylene Resin DOW DMDA-8904 NT 7 is produced using UNIPOL™ process technology. It is intended for use in injection molding applications such as pails, industrial parts and other shipping containers. Information.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6200 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6200 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6220 NT 7 High Density Polyethylene Resin (HDPE) Moderate swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6220 NT 7 is a multipurpose polymer designed for high speed production of blow molded containers used to package househol.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDA-6320 NT 7 High Density Polyethylene Resin (HDPE) Low swell Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDA-6320 NT 7 is a multipurpose polymer designed for the high speed production of blow molded containers used to package household.. |
|||
Melting Point | 131 °C | 268 °F | Dow Method (DSC) |
Dow UNIVAL™ DMDC-6143 NT 7 High Density Polyethylene Resin (HDPE) Excellent parison melt strength / low sag Good extrudability / process-ability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a UNIVAL™ DMDC-6143 NT 7 is a polymer with broad molecular weight distri.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
ExxonMobil HDP8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3418 |
ExxonMobil HD 8760.29 Rotational Molding Resin Product Description: HD 8760 is a high density hexene copolymer designed to offer outstanding stiffness and processability. This resin is ideally suited for applications that require the optimum bal.. |
|||
Melting Point | 131 °C | 268 °F | ASTM D3417 |
Total XT10 N Natural HDPE, pipe Applications: Potable water, industrial and mining, sewer and sewer relining, gas and oil gathering, general pipe relining, pipe coatingInformation provided provided by Total Petrochemicals.Total Pe.. |
|||
Melting Point | 131 °C | 268 °F | DSC |
Formosa Plastics Formolene® E927 Film HDPE High Density Polyethylene High Molecular Weight Bi-Modal Resin For Thin Film Applications Formolene® E927 is a high molecular weight grade of HDPE designed for high drawdown to produce thin films w.. |