Material Notes:
This product is a Total Ecosolutions grade.Lumicene® mPE M5220M is a second generation metallocene high density polyethylene with very good organoleptic properties, dimensional stability, stress-cracking resistance, rigidity and processability.It is especially suited for the production of beverage caps & closures by injection or compression molding, more specifically for carbonated drinks. Other typical applications include caps & closures for cosmetics and general purpose injection-molded articles.This grade contains a slip agent.Information provided by Total Petrochemicals.
Physical Properties Metric English Comments
Specific Gravity 0.952 g/cc
0.952 g/cc
ISO 1183
Melt Flow 2.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.0 MPa
3630 psi
ISO 527
Tensile Modulus 1.00 GPa
145 ksi
ISO 527
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
ISO 11357
Processing Properties Metric English Comments
Melt Temperature <= 250 °C
<= 482 °F