Petromont 2001 High Density Polyethylene Resin

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer Petromont
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Petromont 2001 High Density Polyethylene Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Petromont HDPE 2001 is a high-density polyethylene copolymer resin produced using the UNIPOL ® Process. This resin has been designed specifically for film for various applications such as notion and millinery bags, food packaging, "T-shirt" bags, industrial and agricultural bags, etc.Petromont HDPE 2001 has a broad molecular weight distribution. This, combined with its high molecular weight and balanced density, results in excellent performance at high extrusion rates with high film strength and rigidity. The excellent draw down characteristics permit production of high quality thin films. This product consists of an improved formulation.
Physical Properties Metric English Comments
Density 0.948 g/cc
0.0342 lb/in³
ASTM D1505
Melt Flow 0.070 g/10 min
0.070 g/10 min
I<sub>2</sub>; ASTM D1238
10 g/10 min
10 g/10 min
I<sub>21</sub>; ASTM D238
Thermal Properties Metric English Comments
Melting Point 131 °C
268 °F
Petromont
Vicat Softening Point 124 °C
255 °F
ASTM D1525
Descriptive Properties Value Comments
Process Film