Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 127 - 131 °C | 261 - 268 °F | ISO 3146 |
Polikim ULPOLEN® 300 UHMWPE Standard Standard Ulpolen® 1000 is the universal type primarily preferred on the condition that its technical properties meet operating environment requirements. It is more cost efficient compared to specia.. |
|||
Melting Point | 127 °C | 261 °F | Internal method |
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf.. |
|||
Melting Point | 127 °C | 261 °F | Internal method |
Polimeri Europa Clearflex® FG 336 Hexene Copolymer Linear Low Density Polyethylene Clearflex FG 336 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, slip agent, antiblocking agent and processing aid, suitable for blown film extrusion.Films obtain.. |
|||
Melting Point | 127 °C | 261 °F | Internal method |
Polimeri Europa Clearflex® H&T FHH 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex H&T FHH 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidant, suitable for blown film extrusion.Films obtained from Clearflex H&T FHH 508 show good op.. |
|||
Melting Point | 127 °C | 261 °F | Internal method |
Polimeri Europa Clearflex® RN 50 U Linear Medium Density Polyethylene Clearflex RN 50 U is a linear medium density polyethylene resin, with antioxidants and UV stabilizers, suitable for rotomolding applications.Items manufactured with Clearflex RL 50 U show good mecha.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3417 |
NOVA Chemicals Novapol® TE-0546-GBK Hexene MDPE Extrusion Resin Very good impact, Excellent ESCR, Sub 50 mesh particles sizeApplications: Powder coating of pipes, values, and fittings to produce a corrosion-resistant coating for buried pipe systemsAdditives: Ant.. |
|||
Melting Point | 127 °C | 261 °F | Internal method |
Polimeri Europa Clearflex® CM 406 Hexene Copolymer Linear Low Density Polyethylene Clearflex CM 406 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidants, suitable for cast film extrusion.Films manufactured with Clearflex CM 406 are characterized by h.. |
|||
Melting Point | 127 °C | 261 °F | Internal method |
Polimeri Europa Clearflex® FF 508 Octene Copolymer Linear Medium Density Polyethylene Clearflex FF 508 is an octene copolymer linear medium density polyethylene (C8-LMDPE), with antioxidants and processing aid, suitable for blown film extrusion.Films manufactured with Clearflex FF 50.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LL 8401 Rotational Molding Resin
(discontinued **) LL 8401 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for Non-UV applications that require optimum balance of flow processabil.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LL 8401.67 Rotational Molding Resin
(discontinued **) LL 8401 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for Non-UV applications that require optimum balance of flow processabil.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LL 8450 Rotational Molding Resin
(discontinued **) LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3417 |
Total Finathene® WR 201 B N HDPE blow molding
(discontinued **) FINATHENE® WR 201 B N is a high density polyethylene produced by the slurry loop low pressure polymerization process. FINATHENE® WR 201 B N has been developed for the blow molding of Plastic Fuel .. |
|||
Melting Point | 127 °C | 261 °F | ISO 3146 |
Total Lacqtene® 2003 PBK 41 HDPE pipe, sheet
(discontinued **) LACQTENE® 2003 PBK 41 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer. LACQTENE® 2003 PBK 41 is a black compound especially developed for i.. |
|||
Melting Point | 127 °C | 261 °F | |
LyondellBasell Lupolen® 3652 D SW 00413 MDPE Data was collected by ISO methods and originally provided by BASF. The Lupolen® product line is now produced by Basell. |
|||
Melting Point | 127 - 132 °C | 261 - 270 °F | |
Suqian Unitechem 2,2,6,6-tetramethyl-4-piperidinol Chemical Name: 2,2,6,6-tetramethyl-4-piperidinolCAS NO.: 2403-88-5Molecular Formula: C9H19NOUses: It is an important intermediate of hindered amine light stabilizer and synthetic hindered amine ligh.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D2117 |
SCG Chemicals EL-Leneâ„¢ M90 Butene (C4) Rotational Molding Resin Color compound resin available in pellet / powder formKey Characteristics:High stiffness and toughnessGood ESCRFair processingTypical Applications: Large, thick-wall parts, high-load products, such.. |
|||
Melting Point | 127 °C | 261 °F | DSC; ASTM D3418 |
DuPont Bynel® 4157 Adhesive Resin Bynel® Series 4100 resins are anhydride-modified linear low-density polyethylene (LLDPE) resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment design.. |
|||
Melting Point | 127 °C | 261 °F | ISO 11357 |
Total MDPE HR 515 Medium Density Polyethylene, Blown Film MDPE HR 515 is a medium density polyethylene produced with hexene as a co-monomer. It shows a broad molecular weight distribution ensuring outstanding processability.MDPE HR 515 is especially dedic.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418, ISO 3146 |
DuPont™ Bynel® 41E762 Anhydride Modified LLDPE BYNEL® 41E762 is an anhydride-modified, linear low-density polyethylene (LLDPE) resin. All BYNEL Series 4100 series resins are available in pellet form for use in conventional extrusion and coextru.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LL 8450.31 Rotational Molding Resin Product Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that require.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LL 8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LLP8450.31 Rotational Molding Resin LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LLP8460.29 Rotational Molding Resin Product Description: LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require the optimum balance o.. |
|||
Melting Point | 127 °C | 261 °F | Dow Method (DSC) |
Dow DOWLEX™ 2027G Linear Low Density Polyethylene For high speed, thin gauge applications Improved stiffness Complies with U.S. FDA 21 CFR 177.1520 (c) 3.2a Information provided by Dow |
|||
Melting Point | 127 °C | 261 °F | Dow Method (DSC) |
Dow DOWLEX™ IP-51 High Density Polyethylene Resin (HDPE) DOWLEX™ IP-51 is an Improved Processing high density resin designed to offer excellent process-ability and impact performance. This resin was designed by optimization of the breadth, shape and pea.. |
|||
Melting Point | 127 °C | 261 °F | D.S.C. method |
Arkema Group Orevac® SM7-001-sPP Maleic Anhydride modified Polypropylene Propylene based Main Application: OvermoldingInformation provided by Arkema Group |
|||
Melting Point | 127 °C | 261 °F | Peak Melting Temperature; ExxonMobil Method |
ExxonMobil LL 3404.48 Cast Film Resin
(discontinued **) LL 3404.48 is a hexene medium density polyethylene cast film grade for applications requiring high strength and high stiffness. It can also be used in blown films. Films produced from this resin ex.. |
|||
Melting Point | 127 °C | 261 °F | ISO 3146 |
Total Lacqtene® 2002 TN 40 HDPE, blow molding, pipe, sheet
(discontinued **) LACQTENE® 2002 TN 40 is a high density polyethylene produced by the gas phase polymerization process with hexene as comonomer.Information provided provided by Total Petrochemicals.Total Petrochemic.. |
|||
Melting Point | 127 °C | 261 °F | ASTM D3418 |
ExxonMobil LL 8460 Rotational Molding Resin
(discontinued **) LL 8460 is a linear low density hexene copolymer designed to offer excellent ESCR and toughness. This resin is ideally suited for applications that require optimum balance of stiffness, processabili.. |
|||
Melting Point | 127 °C | 261 °F | Melting point via DSC/ASTM D3418 |
DuPont Bynel® 41E557 Anhydride-Modified LLDPE Adhesive Resin
(discontinued **) Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |